MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mitsubishi Chemical Advanced Materials Fluorosint™ 207 PTFE, Compression Molded Synthetic Mica-filled PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Mica Filled

Material Notes: Food Contact Compliant grade PTFE with a unique combination of dimensional stability and creep resistance, and exceptional sliding and wear properties.

Key Words: Polytetrafluoroethylene
Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.30 g/cc2.30 g/ccASTM D792
Water Absorption at Saturation 0.200 %0.200 %ASTM D570 (17)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 50.050.0ASTM D785
Hardness, Shore D 60.060.0ISO 868
Tensile Strength 10.0 MPa1450 psiISO 527-1/-2 (7)
Elongation at Yield 4.00 %4.00 %ISO 527-1/-2 (7)
Flexural Strength 14.0 MPa2030 psiISO 178 (12)
Compressive Yield Strength  10.5 MPa
@Strain 1.00 %
1520 psi
@Strain 1.00 %
ISO 604 (10)
 15.0 MPa
@Strain 2.00 %
2180 psi
@Strain 2.00 %
ISO 604 (10)
 20.0 MPa
@Strain 5.00 %
2900 psi
@Strain 5.00 %
ISO 604 (10)
Shear Strength 12.0 MPa1740 psiASTM D732
Charpy Impact, Notched 0.750 J/cm²3.57 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square 1.00e+14 ohm1.00e+14 ohmANSI/ESD STM 11.11
Dielectric Constant 2.65
@Frequency 1.00e+6 Hz
2.65
@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 7.87 kV/mm200 kV/inASTM D149
 8.00 kV/mm203 kV/inIEC 60243-1 (15)
Dissipation Factor 0.00800
@Frequency 1.00e+6 Hz
0.00800
@Frequency 1.00e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 103 µm/m-°C57.0 µin/in-°FASTM E-831 (TMA)
 85.0 µm/m-°C
@Temperature 23.0 - 100 °C
47.2 µin/in-°F
@Temperature 73.4 - 212 °F
 90.0 µm/m-°C
@Temperature 23.0 - 150 °C
50.0 µin/in-°F
@Temperature 73.4 - 302 °F
 155 µm/m-°C
@Temperature >=150 °C
86.1 µin/in-°F
@Temperature >=302 °F
Thermal Conductivity 0.440 W/m-K3.05 BTU-in/hr-ft²-°F
Melting Point 327 °C621 °FASTM D3418
Maximum Service Temperature, Air 260 °C500 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C210 °FASTM D648
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Continuous Sunlight AcceptableAcceptable
Hot Water / Steam AcceptableAcceptable
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic AcceptableAcceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters AcceptableAcceptable
 
Descriptive Properties
ESd categoryInsulative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Fluorosint™ 500 PTFE, synthetic mica-filled PTFE, compression molded
Mitsubishi Chemical Advanced Materials Fluorosint™ MT-01 PTFE reinforced with carbon fibers and organometallic fillers
Mitsubishi Chemical Advanced Materials Fluorosint™ 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers
Mitsubishi Chemical Advanced Materials Fluorosint™ HPV PTFE Mica-filled
Mitsubishi Chemical Advanced Materials Ertalyte™ TX Internally Lubricated Semi-Crystalline PET

P1SM09 / 20082

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.