MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Thermal Ceramics Cerafiber® Wet Pack
Categories: Ceramic

Material Notes: Cerafiber Wet Pack is manufactured by combining Cerablanket®, a needled refractory fiber blanket, and inorganic binding agents. Cerafiber Wet Pack is packaged in moist form in polyethylene bags. It is flexible and exhibits high tensile strength in the wet state. When air dried, it becomes a strong, hard, rigid structure.

Two of its most important features include its freeze-thaw stability and no binder migration. It is formulated so that freezing does not significantly affect its strength. In addition, the binder particles do not migrate toward the surface. A rigid, homogenous structure is present throughout the entire material.

Cerafiber Wet Pack can be used for a wide variety of industrial applications. The flexible sheets can be inserted in hard to reach areas. They are easily cut and can be custom molded in complex shapes to a required size, shape and thickness. When the product dries, a hard surface is created. The rigid surface is ideal for service where furnace velocities are of concern.

Features:

  • Refractory use limit, 2400°F (1316°C)
  • Low binder migration
  • Freeze-thaw stability
  • High flexural strength
  • High tensile strength
  • High heat resistance
  • Applications:

  • Pipe wrapping
  • Valve enclosures
  • Flue and stack linings
  • Engine and power plant insulation
  • Hot-face layer where velocity is of concern
  • Catalytic converter wrapping
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 0.0100 g/cc0.000361 lb/in³dry
     0.0236 g/cc0.000853 lb/in³wet
    Thickness 6250 microns246 mil
     12500 microns492 mil
     25000 microns984 mil
     
    Thermal PropertiesMetricEnglishComments
    Specific Heat Capacity 1.087 J/g-°C0.2598 BTU/lb-°F
    Thermal Conductivity  0.0700 W/m-K
    @Temperature 260 °C
    0.486 BTU-in/hr-ft²-°F
    @Temperature 500 °F
     0.100 W/m-K
    @Temperature 538 °C
    0.694 BTU-in/hr-ft²-°F
    @Temperature 1000 °F
     0.160 W/m-K
    @Temperature 816 °C
    1.11 BTU-in/hr-ft²-°F
    @Temperature 1500 °F
     0.220 W/m-K
    @Temperature 1093 °C
    1.53 BTU-in/hr-ft²-°F
    @Temperature 1999 °F

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Hexcel® HexWeb® HRH-10/F35 - 2.5 Nonmetallic Flex-Core Honeycomb
    Hexcel® HexWeb® CFC™-20-1/8-11.0 Composite Flooring Honeycomb Core
    DuPont™ Nomex® 410 Paper, 2 mil Nominal Thickness
    DIAB Rigid Foam IPN 20-649 Type 1
    Covestro Baydur® 683 Polyurethane Structural Foam

    CTHERM014 / 2334

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.