MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
INEOS Styrolution Styrolux® 3G46 SBC
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: Styrolux® 3G46 is a clear styrene-butadiene copolymer (SBC) developed specifically for sheet- and film extrusion and for thermoformed articles. Styrolux® 3G46 is designed for improved performance in blends with general-purpose polystyrene, providing parts with an excellent balance of transparency and toughness. Outstanding clarity, Good toughness / stiffness balance, Medium GPPS blend capability. Applications: Food and non-food packaging, Caps and lids, Toys, Displays, Medical devices, Household products.

Information provided by STYROLUTION, which is a joint venture between BASF and INEOS

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Water Absorption at Saturation 0.070 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0030 - 0.010 cm/cmISO 294-4
Linear Mold Shrinkage, Flow 0.01651 cm/cmASTM D955
Melt Flow 12 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 65ISO 868
Tensile Strength, Yield 27.0 MPaISO 527
Elongation at Break 180 %Nominal; ISO 527
 180 %ISO 527
Elongation at Yield 2.0 %ISO 527
Tensile Modulus 1550 MPaISO 527
Flexural Strength 31.0 MPaISO 178
Flexural Yield Strength 31.0 MPa
@Strain 5.0 %
Flexural Modulus 1550 MPaISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 3.00 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 3.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+15 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.00030
@Frequency 100 Hz
IEC 60250
 0.00080
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 90.0 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 51.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 81.0 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.573Sodium D Line; ISO 489
Haze 1.0 %ASTM 1003
Transmission, Visible 90 %
@Wavelength 550 nm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 250 °CISO 294
Mold Temperature 30.0 - 50.0 °CISO 294
 
Descriptive Properties
Commercial StatusNorth America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Eastar BR203 Copolyester
Overview of materials for Styrene-Butadiene Copolymer, SBC
Chevron Phillips K-Resin® KK38 Styrene-Butadiene Copolymer, Sheet Grade
INEOS Styrolution Styroflex® 2G66 SBC
INEOS Styrolution Styrolux® BX6400 SBC

PBASG0635 / 132268

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.