MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes:

Applications: Wet corrosion resistance and general service.

Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms.

Key Words: EN 1.4318; ASTM 301LN; JIS SUS 301L
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.90 g/ccRT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 765 MPaOutokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
 440 MPa
@Temperature 300 °C
EN min.; EN 10002-5
 460 MPa
@Temperature 200 °C
EN min.; EN 10002-5
 530 MPa
@Temperature 100 °C
EN min.; EN 10002-5
Tensile Strength, Yield 350 MPa
@Strain 0.2 %
EN min., RT; EN 10002-1
 360 MPa
@Strain 0.2 %
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
 395 MPa
@Strain 1 %
Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
 170 MPa
@Strain 0.2 %,
Temperature 300 °C
EN min.; EN 10002-5
 185 MPa
@Strain 0.2 %,
Temperature 200 °C
EN min.; EN 10002-5
 200 MPa
@Strain 1 %,
Temperature 300 °C
EN min.; EN 10002-5
 215 MPa
@Strain 1 %,
Temperature 200 °C
EN min.; EN 10002-5
 265 MPa
@Strain 0.2 %,
Temperature 100 °C
EN min.; EN 10002-5
 300 MPa
@Strain 1 %,
Temperature 100 °C
EN min.; EN 10002-5
Elongation at Break 47 %Outokumpu Typical, Cold Rolled Strip/Sheet; EN 10002-1
Modulus of Elasticity 200 GPaRT
 165 GPa
@Temperature 500 °C
 172 GPa
@Temperature 400 °C
 179 GPa
@Temperature 300 °C
 186 GPa
@Temperature 200 °C
 194 GPa
@Temperature 100 °C
Poissons Ratio 0.30RT
Shear Modulus 77.0 GPacalculated
Impact Test >= 60.0 JHot rolled plate/Cold rolled strip/sheet, 10x10mm test pieces; EN 10045-1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000730 ohm-cmRT
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 100 °C
 16.5 µm/m-°C
@Temperature 200 °C
 17.0 µm/m-°C
@Temperature 300 °C
 17.5 µm/m-°C
@Temperature 400 °C
 18.0 µm/m-°C
@Temperature 500 °C
Specific Heat Capacity 0.500 J/g-°CRT
Thermal Conductivity 15.0 W/m-KRT
 20.0 W/m-K
@Temperature 400 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.020 %
Chromium, Cr 17.7 %
Iron, Fe 75.64 %
Nickel, Ni 6.5 %
Nitrogen, N 0.14 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
301 Stainless Steel
Crucible Steel SUE52 Martensitic Steel
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel

NOUTOK10 / 18725

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.