MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Syncure™ S1010B Polyethylene, Crosslinked (XLPE)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Available as Catalyst Masterbatch component for PolyOne Syncure System.

Oven Aging values are >75, and were measured on a 95 phr S1025A / 5 phr S1010B Syncure System. Pellet appearance is 1/8 cylindrical.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.480 g/ccGeon® 1169; Internal Method
 0.920 g/ccASTM D1505
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
Procedure A; ASTM D1238
 
Descriptive Properties
AppearancePellets/CubesASTM D2090
FormsPellets
Generic MaterialXLPE
Generic NamePolyethylene, Crosslinked (XLPE)
Regional AvailabilityNorth America
Retention of Tensile Elongation75%158°C, 1.91 mm; 168 hr, UL Standard
Retention of Tensile Strength75%158°C, 1.91 mm; 168 hr, UL Standard
UsesWire & Cable Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borlink™ LE4244EHV Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE4201EHV Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE0592S Polyethylene
Avient Syncure™ V0064G Crosslinked Polyethylene (XLPE)
Avient Syncure™ V0045G RoHS Polyethylene, Crosslinked (XLPE)

PH0POL0326 / 144895

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.