MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPR Z9450 Random Copolymer Heat Sealable Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA Z9450 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The very low melting point of ATOFINA Z9450 makes it an excellent heat seal layer for oriented films. Z9450 complies with FDA regulations Title 21 CFR Section 177.150 (c) 3.1 and may be used under these provisions for food contact and packaging.

Application

ATOFINA Z9450 is recommended for use in non-oriented film processes for manufacture of packaging films that require improved optical and impact properties and as a heat seal layer for oriented films.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D1505
Moisture Vapor Transmission 0.472 cc-mm/m²-24hr-atm1.20 cc-mil/100 in²-24hr-atmASTM E96
Melt Flow 5.0 g/10 min5.0 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 17.2 MPa2500 psiASTM D882
1% Secant Modulus 345 MPa50000 psiASTM D882
Dart Drop 10.6 g/micron270 g/milF50; ASTM D1709
Heat Seal Strength Initiation Temperature 112 °C234 °FMinimum seal strength is 200 g/in at 15 psi pressure and 1 sec.; ASTM D1709
 
Thermal PropertiesMetricEnglishComments
Melting Point 129 °C264 °FDSC-2 Differential Scanning Calorimeter
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %ASTM D1003
Gloss 85 %85 %45°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Microthene® MP564189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade
Borealis Bormed™ TD109CF Polypropylene Copolymer

PFINAA077 / 38513

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.