MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene® GA574189 Linear Low Density Polyethylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: PETROTHENE GA574189 exhibits excellent flow and impact with good stiffness. Typical applications include lids, closures, containers, housewares and medical items.

Regulatory Status: GA574189 meets the requirements of the Food and Drug Administration regulation, 21 CFR 1 77.1 520. This regulation allows the use of this olefin polymer in "...articles or components of articles intended for use in contact with food..." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information.

Specific recommendations for processing GA574189 can only be made when the processing conditions, equipment and end use are known.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ASTM D1505
Melt Flow 50 g/10 min50 g/10 minASTM D1238
Spiral Flow 49.0 cm19.3 inEquistar test
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5252ASTM D2240
Tensile Strength at Break 10.3 MPa1500 psiASTM D638
Tensile Strength, Yield 14.5 MPa2100 psi20"/min; ASTM D638
Elongation at Yield 8.2 %8.2 %20"/min; ASTM D638
Flexural Modulus, 1% Secant 441 MPa64000 psi0.5"/min; ASTM D790
2% Secant Modulus 0.414 GPa60.0 ksi0.5"/min; ASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C122 °FASTM D648
Vicat Softening Point 96.0 °C205 °FASTM D1525
Brittleness Temperature <= -76.0 °C<= -105 °FF50; ASTM D746
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 °C350 °F
Middle Barrel Temperature 191 °C375 °F
Front Barrel Temperature 204 °C400 °F
Nozzle Temperature 204 °C400 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow R7021-50RNA Polypropylene Random Copolymer Resin
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade
LyondellBasell Microthene® MP574189 Linear Low Density Polyethylene, Injection Molding Grade
Bamberger Polymers Bapolene® 2292 Polyethylene Film Grade
A. Schulman POLYBATCH™ White L8350 HSF Concentrate Based In High-Flow LLDPE

PEQU0825 / 104181

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.