MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Chemlon® MDT10 Nylon 6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: Notes: MDT10 is a modified nylon 6 that offers ultra high impact strength coupled with good rigidity, with this impact resistance being retained at sub-zero temperatures. The excellent impact performance also means that it may be possible to use moldings prior to any conditioning.

Availability: Europe; North America

Features: High Rigidity; Low Temperature Impact Resistance; Ultra High Impact Resistance

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³ISO 1183
Moisture Absorption at Equilibrium 2.4 %2.4 %50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 42.0 MPa6090 psiISO 527-2
Elongation at Break 140 %140 %ISO 527-2
Tensile Modulus 1.70 GPa247 ksiISO 527-2
Flexural Strength 46.0 MPa6670 psiISO 178
Flexural Modulus 1.60 GPa232 ksiISO 178
Izod Impact, Notched (ISO) NBNBISO 180
Izod Impact, Unnotched (ISO) NBNBISO 180
Charpy Impact Unnotched NBNBISO 179
Charpy Impact, Notched NBNBISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Dielectric Constant 3.13.1IEC 60250
Dielectric Strength 9.84 kV/mm
@Thickness 3.00 mm
250 kV/in
@Thickness 0.118 in
IEC 60243-1
Comparative Tracking Index >= 600 V>= 600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FUnannealed; ISO 72-2/B
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FUnannealed; ISO 72-2/A
Flammability, UL94 HBHB
Oxygen Index 21 %21 %ISO 4589-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 - 280 °C482 - 536 °F
Middle Barrel Temperature 250 - 280 °C482 - 536 °F
Front Barrel Temperature 250 - 280 °C482 - 536 °F
Melt Temperature <= 300 °C<= 572 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F
Dry Time 2.00 hour2.00 hour
Screw Speed 50 - 200 rpm50 - 200 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
W-5Re Type C Tungsten-Rhenium Thermocouple Alloy
W-5 Re Tungsten Rhenium Alloy
Teknor Apex Sarlink® TPV X6170N Thermoplastic Vulcanizate
Teknor Apex Chemlon® E-66 Nylon 66
Mocom (ALBIS) ALTECH® PA6 A 2030/212 GF30 IM UV Nylon 6, 30% Glass Fiber Reinforced

PTEKNQ0612 / 237103

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.