MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV X6170N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV X6170N is a general purpose thermoplastic vulcanizate used in automotive and industrial applications. This product is a medium hardness grade exhibiting superior compression set and chemical resistance. This grade can be processed by injection molding and extrusion.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Flow; Good Processability; Medium Hardness; Low Density; Low Specific Gravity; Resilient

Uses: Automotive Applications; Automotive Interior Parts; Consumer Applications; Industrial Applications; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.929 g/cc0.0336 lb/in³ISO 1183
Viscosity 165 cP
@Shear Rate 206 1/s,
Temperature 200 °C
165 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ISO 11443
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  72
@Time 5.00 sec
72
@Time 0.00139 hour
Extruded; ISO 868
 76
@Time 5.00 sec
76
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 5.40 MPa783 psiFlow; ISO 37
 6.00 MPa870 psiAcross Flow; ISO 37
Tensile Stress at Strain  3.00 MPa
@Strain 100 %
435 psi
@Strain 100 %
Across Flow; ISO 37
 4.30 MPa
@Strain 100 %
624 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 340 %340 %Flow; ISO 37
 510 %510 %Across Flow; ISO 37
Compression Set 46 %
@Temperature 70.0 °C,
Time 79200 sec
46 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 365 - 420 °C689 - 788 °F
Rear Barrel Temperature 180 - 205 °C356 - 401 °F
Middle Barrel Temperature 356 - 401 °C673 - 754 °F
Front Barrel Temperature 356 - 401 °C673 - 754 °F
Nozzle Temperature 365 - 410 °C689 - 770 °F
Mold Temperature 50.0 - 120 °C122 - 248 °F
Back Pressure 0.100 - 1.00 MPa14.5 - 145 psi
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
AppearanceNatural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
W-5Re Type C Tungsten-Rhenium Thermocouple Alloy
W-5 Re Tungsten Rhenium Alloy
Teknor Apex Chemlon® MDT10 Nylon 6
Teknor Apex Chemlon® E-66 Nylon 66
Mocom (ALBIS) ALTECH® PA6 A 2030/212 GF30 IM UV Nylon 6, 30% Glass Fiber Reinforced

PTEKNQ1217 / 237708

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.