CS 7979* is used for reinforcement of high-temperature thermoplastics. It was especially developed for PPS. This type can also be used for other polymers e.g. PA 12, PPO. Very high mechanical strength; High resistance to hydrolysis and Reduced generation of volatiles during injection-molding Information provided by Lanxess. |