MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lanxess CS 7979 Glass Fiber
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: CS 7979* is used for reinforcement of high-temperature thermoplastics. It was especially developed for PPS. This type can also be used for other polymers e.g. PA 12, PPO.

Very high mechanical strength; High resistance to hydrolysis and Reduced generation of volatiles during injection-molding

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Absorption <= 0.050 %<= 0.050 %
 
Descriptive Properties
Specifications0.4 percentSize content
 10 µmFiber Diameter
 4.5 mmAv. Fiber Length

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A-Glass Fiber, Generic
Hexcel® HexTow® AS4C 6K Standard Modulus Carbon Fiber (6000 Filaments)
Hexcel® HexTow® AS4 3K Standard Modulus Carbon Fiber (3000 Filaments)
Hexcel® HexForce™ 220HT Fiber Glass Fabric
Fiberglass Grade B

PLANY8658 / 209051

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.