  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

(Viewing data as-entered. Click here to return)
Titanium, high purity
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes:

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.51 g/ccalpha
 4.35 g/cc
@Temperature 885 °C
beta
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 90increases with impurities
Hardness, Knoop 99Estimated from Brinell.
Hardness, Vickers 100increases with impurities
Modulus of Elasticity 105 GPa
Poissons Ratio 0.32 - 0.36
Fatigue Strength 130 MPa
@# of Cycles 1.00e+6
Shear Modulus 39.2 GPaCalculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000450 ohm-cm
Magnetic Susceptibility 0.00000317cgs/g
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 325 J/g
CTE, linear 8.41 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.523 J/g-°C
Thermal Conductivity 17.0 W/m-K
Melting Point 1670 °C
Liquidus 1660 °C
Beta Transus 882 °CHeat of transition is 85 J/g
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.30
@Temperature 710 °C
Reflection Coefficient, Visible (0-1) 0.56Visible
 
Component Elements PropertiesOriginal ValueComments
Titanium, Ti 100 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Titanium Grade 1
Titanium Grade 2
Titanium Grade 7
Titanium Grade 3
Titanium Grade 11

MTUHP0 / 14270

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.