MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Titanium Grade 1
Categories: Metal; Nonferrous Metal; Titanium Alloy; Unalloyed/Modified Titanium

Material Notes: Information provided by Allvac and the references.

Characteristics: Higher ductility, Lower strength, Greater corrosion resistance - when compared to alloys, Weldable

Applications: Airframe components, cryogenic vessels, heat exchangers, CPI equipment, condenser tubing, pickling baskets.

Forms typically available: billet, bar, plate, sheet, strip, rod, wire, extrusions, tubing.

Titanium Grades 1,2,3,4,7,11,and 12 are all considered unalloyed and have similar mechanical properties.

Key Words: UNS R50250; ASTM Grade 1, CP titanium, C.P. titanium alloy
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 4.50 g/cc0.163 lb/in³
a Lattice Constant  2.95 Å
@Temperature 25.0 °C
2.95 Å
@Temperature 77.0 °F
alpha phase
 3.29 Å
@Temperature 900 °C
3.29 Å
@Temperature 1650 °F
beta phase
c Lattice Constant 4.683 Å
@Temperature 25.0 °C
4.683 Å
@Temperature 77.0 °F
c/a = 1.587
 
Chemical PropertiesMetricEnglishComments
Thermal Neutron Cross Section 5.6 barns/atom5.6 barns/atomAverage for naturally occurring Ti
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 120120annealed
Hardness, Knoop 132132Estimated from Brinell.
Hardness, Rockwell B 7070annealed
Hardness, Vickers 122122Estimated from Brinell.
Tensile Strength  124 - 138 MPa
@Temperature 427 °C
18000 - 20000 psi
@Temperature 801 °F
 152 - 179 MPa
@Temperature 316 °C
22000 - 26000 psi
@Temperature 601 °F
 193 - 207 MPa
@Temperature 204 °C
28000 - 30000 psi
@Temperature 399 °F
Tensile Strength, Ultimate 240 MPa34800 psi
Tensile Strength, Yield 170 - 310 MPa24700 - 45000 psi
 76.0 - 90.0 MPa
@Temperature 427 °C
11000 - 13100 psi
@Temperature 801 °F
0.2% offset
 83.0 - 103 MPa
@Temperature 316 °C
12000 - 14900 psi
@Temperature 601 °F
0.2% offset
 110 - 124 MPa
@Temperature 204 °C
16000 - 18000 psi
@Temperature 399 °F
0.2% offset
Elongation at Break 24 %24 %
 25 - 30 %
@Temperature 427 °C
25 - 30 %
@Temperature 801 °F
 30 - 35 %
@Temperature 316 °C
30 - 35 %
@Temperature 601 °F
 40 - 50 %
@Temperature 204 °C
40 - 50 %
@Temperature 399 °F
Reduction of Area 35 %35 %
Tensile Modulus 103 GPa14900 ksi
Compressive Modulus 110 GPa16000 ksi
Poissons Ratio 0.370.37
Shear Modulus 45.0 GPa6530 ksi
Charpy Impact 310 J229 ft-lbV-notch
Impact Test 136 J100 ft-lbImpact Strength
Coefficient of Friction, Dynamic 0.680.68Ti sliding on Ti; 300 m/min
 0.800.80Ti sliding on Ti; 40 m/min
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000420 ohm-cm0.0000420 ohm-cm
Magnetic Permeability 1.000051.00005at 1.6 kA/m
Magnetic Susceptibility 3.98e-83.98e-81/kg; Paramagnetic
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 325 J/g140 BTU/lbHigh Purity Ti.
CTE, linear  8.35 µm/m-°C
@Temperature 15.0 °C
4.64 µin/in-°F
@Temperature 59.0 °F
 8.70 µm/m-°C
@Temperature 100 °C
4.83 µin/in-°F
@Temperature 212 °F
 9.50 µm/m-°C
@Temperature 300 °C
5.28 µin/in-°F
@Temperature 572 °F
 9.70 µm/m-°C
@Temperature 0.000 - 540 °C
5.39 µin/in-°F
@Temperature 32.0 - 1000 °F
perpendicular to the c-axis
Specific Heat Capacity 0.520 J/g-°C0.124 BTU/lb-°F
 0.560 J/g-°C
@Temperature 200 °C
0.134 BTU/lb-°F
@Temperature 392 °F
 0.620 J/g-°C
@Temperature 400 °C
0.148 BTU/lb-°F
@Temperature 752 °F
 0.690 J/g-°C
@Temperature 600 °C
0.165 BTU/lb-°F
@Temperature 1110 °F
Thermal Conductivity 16.0 W/m-K111 BTU-in/hr-ft²-°Fannealed
Melting Point <= 1670 °C<= 3040 °F
Liquidus 1670 °C3040 °F
Beta Transus 882 °C1620 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.30
@Temperature 710 °C
0.30
@Temperature 1310 °F
High purity Ti
Reflection Coefficient, Visible (0-1) 0.560.56High purity Ti; visible light.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.10 %<= 0.10 %
Hydrogen, H <= 0.015 %<= 0.015 %
Iron, Fe <= 0.20 %<= 0.20 %
Nitrogen, N <= 0.030 %<= 0.030 %
Other, total <= 0.30 %<= 0.30 %
Oxygen, O <= 0.18 %<= 0.18 %
Titanium, Ti >= 99.175 %>= 99.175 %
 
Descriptive Properties
Alpha Phase Crystal Structurecph, below 882°C
Beta Phase Crystal Structurebcc, above 882°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 2
Silicon Nitride
Titanium Grade 1, Annealed
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Titanium Grade 4

MTU010 / 14257

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.