MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient reFlex™ 100 Plasticizer, Bio-derived
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Bio-derived, non-phthalate plasticizer; USDA BioPreferred® certified 94% biobased.

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.947 - 0.953 g/cc
@Temperature 25.0 °C
ASTM D4052
Molecular Weight 316 g/molTheoretical, approximate
ASTM Color <= 50Pt-Co Scale; ASTM D1209
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 1.0[mg KOH/g]; ASTM D1045
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.15 %ASTM E1064
 
Descriptive Properties
Agency RatingsUSDA Certified Biobased Product
AppearanceClear, cleanASTM D2090
 Clear/Transparent
FeaturesFast Fusion
 Fast Gel
 High Solvating
 Non-Phthalate Plasticizer
 Renewable Resource Content
FormsLiquid
Generic MaterialPlasticizer, Bio-derived
Generic NamePlasticizer, Bio-derived
Hydroxyl Value< 20.0 mg KOH/gAOCS Tx 1a-66
Oxirane Content> 6.9 wt%ASTM D1652
Processing MethodCompounding
 Hot Melt
 Plastisol
Regional AvailabilityNorth America
UsesCarpet Backing
 Consumer Applications
 Fabric Coatings
 Flooring
 Foam
 Printing Ink
 Sealants
 Sporting Goods
 Toys

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wieland Porta REFLEX® PFM Alloy
Struktol TR 255 Processing Additive, Dispersant
Struktol TR 251 Processing Additive, Dispersant
Struktol TR 045 Processing Additive
Struktol TR 041 Processing Additive

PH0POL1364 / 145933

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.