MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Struktol TR 041 Processing Additive
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Oleochemical derivative with no metal ions.

STRUKTOL® TR 041 is a fatty acid based additive designed to maximize the wetting to both a polar filler and a non-polar polymer. By wetting both surfaces, this material allows a quicker incorporation of additives into the polymer matrix; decreasing mixing times, melt temperatures and viscosity. This product contains no metal soaps and may be used where these are unacceptable. The acid value is quite low, so this compound may also be used where stearic acid is a problem. Specific viscosity improvements have been seen with high impact polystyrene (HIPS).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.980 g/cc0.980 g/cc
Additive Loading 0.10 - 1.0 %0.10 - 1.0 %Depending on polymer and other additives
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 20<= 20
 
Thermal PropertiesMetricEnglishComments
Dropping Point 78.0 - 92.0 °C172 - 198 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life >= 24.0 Month>= 24.0 Month
 
Descriptive Properties
AppearanceLight tan beads or pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Struktol TR 065 Blending Aid, Processing Additive
Struktol TR 121 Slip Agent, Lubricant, Mold Release Agent
Struktol TR 060 Blending Aid, Processing Additive
Struktol TR 071 Processing Additive
Struktol TR 045 Processing Additive

PSTRUK01 / 69229

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.