Turco Liquid Alumigold C is an acidic liquid product used to produce a chromate conversion coating on aluminum and all its alloys. Turco Liquid Alumigold C is non-complex cyanide-accelerated, and it is applied by immersion or spray applications to produce lighter colorless or heavier-colored coatings. |
Aerospace Surface Treatment |