MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Henkel Turco Deoxidizer 6 Makeup / 16 Replenisher Deoxidizer
Categories: Fluid; Solvent

Material Notes: The Turco Deoxidizer 6 / 16 process primarily utilizes two liquid products, Deoxidizer 6 Makeup and Deoxidizer 16 Replenisher. These are added to either dilute nitric acid or dilute sulfuric acid to produce an efficient production bath for the deoxidizing, desmutting or acid etching aluminum and its alloys.
    Applications:
  • Deoxidizer/Desmutter
  • Conversion Coatings
  • Boric Sulfuric Anodizing
  • Chromic Acid Anodizing
  • Phosphoric Acid Anodizing

Key Words: Aerospace Surface Treatment
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
ChemistryChromated
ConsistencyLiquid
FormConcentrated, Two Part
SubstrateAluminum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Henkel Turco 5948-R Deoxidizer
Henkel Turco 5668 Deoxidizer
Henkel Turco D HX-357 Make-Up and Replenisher Deoxidizer
Henkel Turco Aldox V Deoxidizer
Henkel Turco Liquid Alumigold C Conversion Coating

PHENK889 / 146894

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.