MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® 64C-R Nylon 66, Extrusion Grade
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Extruded

Material Notes: Vydyne 64C-R is a medium-viscosity PA66 resin suitable for injection-molding, extrusion and compounding applications. It is available in natural color only. 64C-R resin offers high strength, rigidity and toughness over a broad range of demanding applications and good fluid resistance to a wide variety of chemicals, solvents and oils.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDAM; ISO 1183
Moisture Absorption at Equilibrium 2.5 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 8.5 %ISO 62
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Dielectric Strength 23.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
Arc Resistance 60 - 120 sec
@Thickness 3.00 mm
PLC 6; ASTM D 495
Comparative Tracking Index 600 V
@Thickness 3.00 mm
IEC 60112
Hot Wire Ignition, HWI 7.0 - 15 secPLC 4; UL 746
 15 - 30 secPLC 3; UL 746
High Amp Arc Ignition, HAI >= 120 arcsPLC 0; UL 746
 >= 120 arcsPLC 0; UL 746
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/minUL 746
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 100 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 260 °CDAM; ISO 11357-3
UL RTI, Electrical 130 °C
@Thickness 1.50 mm
UL 746
 130 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 75.0 °C
@Thickness 1.50 mm
UL 746
 75.0 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 85.0 °C
@Thickness 1.50 mm
UL 746
 85.0 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 V-2
@Thickness 1.50 mm
 V-2
@Thickness 3.00 mm
Glow Wire Ignition Temperature 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 800 °C
@Thickness 1.50 mm
IEC 60695-2-12
 850 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Zone 1 250 - 295 °CExtrusion
Zone 2 250 - 295 °CExtrusion
Zone 3 250 - 295 °CExtrusion
Zone 4 250 - 295 °CExtrusion
Zone 5 250 - 295 °CExtrusion
Die Temperature 270 - 295 °CExtrusion
Melt Temperature 270 - 295 °CExtrusion
 
Descriptive Properties
Agency RatingsASTM, D4066 PA0112
 ASTM, D6779 PA0112
 EC, 1935/2004
 EU, 10/2011
 EU, 2023/2006
AppearanceNatural Color
FeaturesChemical Resistant
 General Purpose
 Good Toughness
 High Melt Strength
 High Rigidity
 High Strength
 Medium Viscosity
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodOther Extrusion
RegionNorth America, Europe, Asia Pacific
UL File NumberE70062

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos Nova 5100 High Impact Polystyrene
Ineos Nova 464 High Impact Polystyrene Injection Molding Grade
Ineos Nova 4250 High Impact Polystyrene Injection Molding Grade
Celanese Nilit FRIANYL A63 S Nylon 6.6 for injection molding
Bamberger Polymers Bapolan® 6409 Polystyrene, Injection Grade

PASCE9755 / 220858

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.