High impact, Medium flow Applications: General purpose injection molding items, Coat hangers, Industrial items This grade complies with European, German, and US food standards. Properties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified. Information provided by NOVA Chemicals. INEOS NOVA began October 1 2007 as an expansion of the 50:50 joint venture between NOVA Chemicals and INEOS to include North American assets. |