MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Axiall 5006 Rigid PVC, Extrusion, White  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf 5006 White is a rigid PVC pellet compound designed for extrusion of rigid PVC house siding, window profiles and various contours where maximum weather resistance is required. Georgia Gulf 5006 White is widely used for window profiles and house siding. Twin screw extruded sheet and kick panels are also produced. USDA approval allows 5006 to be used for walk-in cooler walls, refrigerated truck panels and associated profiles. Single or twin screw machines may be used to convert Georgia Gulf 5006 White. It has been designed with excellent impact at ambient temperatures. The high flexural and tensile strength makes it highly suitable for structural installation. The extrusion flow characteristics are excellent, and complicated panel profiles are easily filled out, requiring a minimum of pull-down.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.45 g/ccASTM D-792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 116ASTM D-785
Hardness, Shore D 82ASTM D-2240
Tensile Strength, Yield 7100 psiASTM D-638
Tensile Modulus 450000 psiASTM D-638
Flexural Strength 12200 psiASTM D-790
Flexural Modulus 500000 psiASTM D-790
Izod Impact, Notched 1.50 ft-lb/in
@Thickness 6.35 mm
ASTM D-256
 2.50 ft-lb/in
@Thickness 3.17 mm
ASTM D-256
Tensile Impact Strength 65.0 ft-lb/in²ASTM D-1822
 
Thermal PropertiesOriginal ValueComments
CTE, linear 36.0 µin/in-°F
@Temperature 20.0 °C
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 156 °FASTM D-648
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Melt Temperature 365 °F
 
Compliance PropertiesOriginal ValueComments
USDA Yes
 
Descriptive Properties
Cell Classification13464ASTM D-1784

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 3121 Rigid PVC, Extrusion
Axiall 3101 Rigid PVC, Extrusion
Axiall 7555 Rigid PVC, Extrusion, White
Geon® Performance Solutions x150-206-14702 Vinyl Compound - Rigid (RPVC)
Avient Polytron® 79837 Vinyl Compound - Rigid (RPVC)

PGGUL395 / 41671

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.