MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Axiall 3121 Rigid PVC, Extrusion  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is suitable for such applications as windows, doors, decks and fencing.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.50 g/cc1.50 g/ccASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D-785
Hardness, Shore D 8282ASTM D-2240
Tensile Strength, Yield 45.0 MPa6530 psiASTM D-638
Elongation at Yield 4.2 %4.2 %ASTM D-638
Tensile Modulus 2.72 GPa395 ksiASTM D-638
Flexural Strength 76.46 MPa11090 psiASTM D-790
Flexural Modulus 2.54 GPa368 ksiASTM D-790
Izod Impact, Notched  2.30 J/cm
@Thickness 6.35 mm
4.30 ft-lb/in
@Thickness 0.250 in
ASTM D-256
 11.2 J/cm
@Thickness 3.17 mm
21.0 ft-lb/in
@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 210 kJ/m²100 ft-lb/in²ASTM D-1822
 
Thermal PropertiesMetricEnglishComments
CTE, linear 63.0 µm/m-°C
@Temperature 20.0 °C
35.0 µin/in-°F
@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 69.4 °C157 °FASTM D-648
 
Descriptive Properties
Cell Classification13343ASTM D-1784
 14434323ASTM D-4216

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall 7555 Rigid PVC, Extrusion, White
Axiall 5006 Rigid PVC, Extrusion, White
Axiall 3101 Rigid PVC, Extrusion
Geon® Performance Solutions x150-206-14702 Vinyl Compound - Rigid (RPVC)
Avient Polytron® 79837 Vinyl Compound - Rigid (RPVC)

PGGUL376 / 41652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.