MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Mitsubishi Chemical Advanced Materials Borotron® HD050 5% Boron-filled Polyethylene (ASTM Product Data Sheet)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7171ASTM D2240
Tensile Strength 16.60 MPa2407 psiASTM D638
Tensile Strength at 65°C (150°F) 2.76 MPa400 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Tensile Modulus 0.7667 GPa111.2 ksiASTM D638
Flexural Strength 29.1 MPa4220 psiASTM D790
Flexural Modulus 0.8729 GPa126.6 ksiASTM D790
Compressive Strength 6.60 MPa957 psi10% Def.; ASTM D695
 11.70 MPa1697 psi2% Def.; ASTM D695
 19.1 MPa2770 psi5% Def.; ASTM D695
 24.50 MPa3553 psi10% Def.; ASTM D695
Compressive Modulus 0.6718 GPa97.44 ksiASTM D695
Izod Impact, Notched 0.481 J/cm0.900 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+12 ohm>= 1.00e+12 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 198 µm/m-°C
@Temperature -40.0 - 150 °C
110 µin/in-°F
@Temperature -40.0 - 302 °F
ASTM E831
Melting Point 128 °C262 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C116 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
3A-Dairy NoNo
Canada AG NoNo
FDA NoNo
NSF NoNo
USDA NoNo
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) AcceptableAcceptable
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents UnacceptableUnacceptable
Conductive / Static Dissipative YesYes
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic UnacceptableUnacceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters UnacceptableUnacceptable

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
PTS Trilac® ABS-HF5500 High Flow ABS Resin
PTS Trilac® FR3800-V Flame Retardant ABS Resin, RoHS Compliant
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Mitsubishi Chemical Advanced Materials TIVAR™ 1000 Virgin UHMW-PE, (Natural & Colors except Black)
Bamberger Polymers Bapolene® 0760 High Density Polyethylene, Blow Molding Grade

P1SM52 / 85179

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.