MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.930 g/cc0.930 g/ccASTM D792
Water Absorption <= 0.010 %<= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %<= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ASTM D2240
Tensile Strength 40.0 MPa5800 psiASTM D638
Tensile Strength at 65°C (150°F) 2.76 MPa400 psiASTM D638
Elongation at Break 300 %300 %ASTM D638
Tensile Modulus 0.552 GPa80.0 ksiASTM D638
Flexural Strength 24.1 MPa3500 psiASTM D790
Flexural Modulus 0.600 GPa87.0 ksiASTM D790
Compressive Strength 20.7 MPa3000 psi10% Def.; ASTM D695
Compressive Modulus 0.552 GPa80.0 ksiASTM D695
Shear Strength 33.1 MPa4800 psiASTM D732
Izod Impact, Notched NBNBASTM D256 Type A
Coefficient of Friction, Dynamic 0.120.12Dry vs. Steel; QTM55007
Sand Slurry 10101018 Steel = 100
Limiting Pressure Velocity 0.105 MPa-m/sec3000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square >= 1.00e+15 ohm>= 1.00e+15 ohmASTM D257
Dielectric Constant 2.3
@Frequency 1e+6 Hz
2.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 90.6 kV/mm2300 kV/inShort Term; ASTM D149
Dissipation Factor 0.00050
@Frequency 1e+6 Hz
0.00050
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 198 µm/m-°C
@Temperature -40.0 - 149 °C
110 µin/in-°F
@Temperature -40.0 - 300 °F
ASTM E831
Thermal Conductivity 0.409 W/m-K2.84 BTU-in/hr-ft²-°F
Melting Point 135 °C275 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 82.2 °C180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 46.7 °C116 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Estimated Rating
 
Compliance PropertiesMetricEnglishComments
3A-Dairy YesYesNATURAL ONLY, not colors
Canada AG YesYesNATURAL ONLY, not colors
FDA YesYes
NSF NoNo
USDA YesYes
USP Class VI NoNo
 
Chemical Resistance PropertiesMetricEnglishComments
Acids, Strong (pH 1-3) LimitedLimited
Acids, Weak AcceptableAcceptable
Alcohols AcceptableAcceptable
Alkalies, Strong (pH 11-14) AcceptableAcceptable
Alkalies, Weak AcceptableAcceptable
Chlorinated Solvents AcceptableAcceptable
Conductive / Static Dissipative NoNo
Continuous Sunlight LimitedLimited
Hot Water / Steam LimitedLimited
Hydrocarbons - Aliphatic AcceptableAcceptable
Hydrocarbons - Aromatic UnacceptableUnacceptable
Inorganic Salt Solutions AcceptableAcceptable
Ketones, Esters LimitedLimited
 
Descriptive Properties
ColorNatural
Machinability31-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
Mitsubishi Chemical Advanced Materials TIVAR® ECO UHMW-PE, Recycled (ASTM Product Data Sheet)
Overview of materials for High Density Polyethylene (HDPE), Extruded
Overview of materials for High Density Polyethylene (HDPE), Injection Molded

P1SMP00 / 20148

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.