Description: Breather fabric. Ideally suited to high temperature applications. Features & Benefits: - Nylon 66, non-woven felt which operates at temperatures up to 232°C (450°F) without trapping off air flow
- Available in 225, 339, 369g/m2 (6, 10 and 13oz/yd2) for withstanding pressure to over 200 psi (13.8bar)
- Resists compression and heat set as experienced by other lower temperature resistant fibers.
Information provided by Cytec, subsequently acquired by Solvay. |