MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Circalok™ 6744 A/B Silicone Rubber Compound
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Circalok™ 6744 A/B is a low cost, low viscosity, flame retardant, room temperature curing silicone rubber compound. Circalok™ 6744 meets UL's 94V-0 rating in testing at LORD Laboratories. Mix ratio by weight or volume is 1 to 1. Cures at room temperature in less than 2 hours or at 65°C in a few minutes.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.37 g/cccured
Viscosity 2500 cP
@Temperature 25.0 °C
Part B
 2700 cP
@Temperature 25.0 °C
Mixed
 3000 cP
@Temperature 25.0 °C
Part A
Linear Mold Shrinkage 0.0040 in/incured
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 55cured
Tensile Strength 400 psicured
Elongation at Break 100 %cured
Tear Strength 3.51 kN/mdie B
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmcured
Dielectric Constant 3.2
@Frequency 100 Hz
cured
Dielectric Strength 450 V/milcured
Dissipation Factor 0.0050
@Frequency 100 Hz
cured
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.360 W/m-Kcured
Maximum Service Temperature, Air 205 °Ccured
Minimum Service Temperature, Air -55.0 °C
Flammability, UL94 V-0
 
Processing PropertiesOriginal ValueComments
Cure Time 0.750 hour
@Temperature 65.0 °C
Pot Life 15.0 min
@Temperature 25.0 °C
Shelf Life 6.00 Montheach component, from date of shipment in closed container
 
Descriptive Properties
AppearanceBlackPart A
 GreyMixed
 WhitePart B
Mixed Appearance100 to 100A/B, by weight or by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9280 / 232636

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.