Circalok™ 6744 A/B is a low cost, low viscosity, flame retardant, room temperature curing silicone rubber compound. Circalok™ 6744 meets UL's 94V-0 rating in testing at LORD Laboratories. Mix ratio by weight or volume is 1 to 1. Cures at room temperature in less than 2 hours or at 65°C in a few minutes.All information provided by Lord. |