- Quenched and tempered for uniformity in strength, shock resistance, ductility and hardness.
- Versatile machinery steel.
- Furnished in a hot rolled state.
- Minimum: 125 ksi yield.
- Hardness: 287 – 332 BHN.
- Mechanical properties at 1” below surface.
Information provided by Astralloy, a Nucor Company. |