MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger Tecamid® 6/6 Nylon (PA66)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Type 6/6 is a general purpose standard grade nylon. Extruded in natural and black. (Weather Resistant Black Grade is also available.)

Information Provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.0412 lb/in³ASTM D792
Water Absorption 1.2 %at 24 hours; ASTM D570
Water Absorption at Saturation 8.5 %ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ASTM D785
Tensile Strength, Yield 11600 psiASTM D638
Elongation at Break 25 %ASTM D638
Tensile Modulus 350000 psiASTM D638
Flexural Strength 15500 psiASTM D790
Flexural Modulus 440000 psiASTM D790
Compressive Strength 5000 psiASTM D695
Izod Impact, Notched 1.10 ft-lb/inASTM D256
Coefficient of Friction, Dynamic 0.2640 psi, 50 fpm; ASTM D3702
K (wear) Factor 200 x 10-10 in³-min/ft-lb-hr40 psi, 50 fpm; ASTM D3702
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.6
@Frequency 1e+6 Hz
ASTM D150
 4.0
@Frequency 60 Hz
ASTM D150
Dielectric Strength 300 - 400 V/milASTM D149
Dissipation Factor 0.010
@Frequency 60 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 45.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Specific Heat Capacity 0.400 BTU/lb-°F
Melting Point 491 °FASTM D2133
Maximum Service Temperature, Air 185 °FLong Term; ASTM UL746B
 300 °FIntermittent
Deflection Temperature at 0.46 MPa (66 psi) 455 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 194 °FASTM D648
Flammability, UL94 V-2
@Thickness 3.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 66/6
BASF Ultramid® A3K PA66 (Dry)
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 66, Extruded

PENS69 / 35994

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.