MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem GM7040G HDPE High Density Extrusion Polyethylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: GM7040G is a high-density polyethylene compound specially developed for the manufacturing of extruded pipes for a gas pressurized line. It is produced with bimodal technology and has high molar mass. It shows high mechanical properties and has excellent resistance to hydrostatic pressure and to stress cracking. The resin has the MRS (Minimum Required Strength) of 8 MPa according to ISO 9080 and is classified as PE 80 according to ISO 12162. GM7040G is manufactured in a yellow color and contains additives to protect it against ultraviolet radiation action and photodegradation. Its applications include yellow PE 80 pressure pipes for gas distribution and jacketing of underwater cables.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.947 g/ccASTM-D792
ESCR 100% Igepal® >= 1000 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
0.3 mm notched-plaques; ASTM-D1693
Melt Flow 0.45 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM-D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 62ASTM-D2240
Tensile Strength at Break 37.0 MPaASTM-D638
Tensile Strength, Yield 23.0 MPaASTM-D638
Elongation at Break 770 %ASTM-D638
Elongation at Yield 9.2 %ASTM-D638
Flexural Modulus, 1% Secant 1080 MPaASTM-D790
Izod Impact, Notched 240 J/mASTM-D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CASTM-D648
Vicat Softening Point 122 °C
@Load 1.02 kg
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Braskem GM8250T HDPE High Density Extrusion Polyethylene
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin
Braskem GP100OR HDPE High Density Extrusion Polyethylene
Chevron Phillips Marlex® HXM 50100 Extra high molecular weight hexene copolymer

PBRAS810 / 106656

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.