MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601

Applications:Base Resin for use in Utility and Conduit Pipe Applications

Data provided by Chevron Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.945 g/cc0.0341 lb/in³ASTM D1505
Environmental Stress Crack Resistance  >= 1200 hour
@Temperature 50.0 °C
>= 1200 hour
@Temperature 122 °F
F 0 (25% Igepal); ASTM D1693
 >= 2000 hour
@Temperature 50.0 °C
>= 2000 hour
@Temperature 122 °F
F50, Cond. B.; ASTM D1693
ESCR 100% Igepal® >= 2000 hour
@Temperature 100 °C
>= 2000 hour
@Temperature 212 °F
F 0; ASTM D1693
High Load Melt Index 11 g/10 min
@Load 21.6 kg,
Temperature 190 °C
11 g/10 min
@Load 47.6 lb,
Temperature 374 °F
High Load; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6666ASTM D2240
Tensile Strength, Ultimate 34.0 MPa4930 psiASTM D638
Tensile Strength, Yield 22.0 MPa3190 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus 0.900 GPa131 ksi3 pt. secant. ASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 57.0 °C135 °FASTM D648
Vicat Softening Point 126 °C259 °FASTM D1525
Brittleness Temperature <= -59.0 °C<= -74.2 °FASTM D746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem GM8250T HDPE High Density Extrusion Polyethylene
Borealis BorSafe™ HE3490-LS Black High Density Polyethylene for Pressure Pipes
Braskem GM7040G HDPE High Density Extrusion Polyethylene
Versalis Eraclene® PF 92 High Density Polyethylene - Pipe Grade Resin
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin

PCHEVV53 / 20449

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.