MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ChevronTexaco RPM® SAE 50 Synthetic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Features

Chevron RPM Synthetic Transmission Fluid is a heavy duty truck manual transmission fluid.

It is manufactured from synthesized hydrocarbon base fluids which have excellent thermal and oxidation stability, a high natural viscosity index, and a very low pour point.

This product possesses excellent shear stability even under heavily loaded conditions.

The low pour point and low temperature fluidity of Chevrons RPM Synthetic Transmissions Fluid imparts improved lubrication during startup at subzero temperatures, while the improved viscosity-temperature characteristics provide dependable lubrication at high temperatures. Lower frictional losses in the lubricant film and reduced churning losses, due to lower bulk oil viscosity, reduce operating temperatures significantly when compared to conventional mineral based lubricants.

Applications

Chevron RPM Synthetic Transmission Fluid’s outstanding low temperature flow properties and natural high viscosity index provides superior all-climate, year-round performance in heavy duty truck transmissions.

Its use permits easier shifting in extremely cold weather and less drag and gear wear during startup.

This product is not recommended for use as an engine crankcase oil.

Key Words: CPS Number: 210456; MSDS Number: 4896
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
API Gravity 30.9 °30.9 °
Brookfield Viscosity  1250 cP
@Temperature 0.000 °C
1250 cP
@Temperature 32.0 °F
 3850 cP
@Temperature -10.0 °C
3850 cP
@Temperature 14.0 °F
 11650 cP
@Temperature -20.0 °C
11650 cP
@Temperature -4.00 °F
 14250 cP
@Temperature -26.0 °C
14250 cP
@Temperature -14.8 °F
 45250 cP
@Temperature -30.0 °C
45250 cP
@Temperature -22.0 °F
 270000 cP
@Temperature -40.0 °C
270000 cP
@Temperature -40.0 °F
Viscosity Measurement 144144Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 685 SUS685 SUS
Saybolt Viscosity at 210°F 90 SUS90 SUS
Kinematic Viscosity at 40°C (104°F) 133 cSt133 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 17.4 cSt17.4 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -48.0 °C-54.4 °FASTM D97
Flash Point 228 °C442 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid
Phillips 66 Triton® Heavy Duty ATF Automatic Transmission Fluid
Phillips 66 Kendall® Classic ATF Transmission Fluid
Phillips 66 CVT Fluid Full-Synthetic Transmission Fluid
ELM® SoyFluid™ Hydraulic Universal Tractor Biodegradable Tractor Hydraulic-Transmission Fluid

WCHEV049 / 74664

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.