MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips 66 Triton® Heavy Duty ATF Automatic Transmission Fluid
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Triton Heavy Duty ATF is a full-synthetic, heavy-duty automatic transmission fluid designed for use in truck and bus transmissions operating under severe service conditions or in extended drain intervals. It is particularly recommended by Phillips 66 Company for use in applications where the OEM specifies a fluid providing performance capability comparable to the Allison TES- 295 specification. Triton Heavy Duty ATF has excellent shear stability and high load-carrying ability to protect against viscosity breakdown and wear. It has excellent oxidation resistance and thermal stability to minimize the formation of sludge and varnish, and excellent friction durability to ensure smooth shifting and proper transmission performance for the life of the fluid. It also has outstanding low-temperature properties for year-round use, and protects against rust and corrosion. Triton Heavy Duty ATF can provide extended drains up to 4 times the normal interval for a conventional all-mineral automatic transmission fluid. It was field tested for over 100,000 miles in a fleet of city transit buses operating in severe stop-and-go service. During this test, it provided outstanding protection against wear, glazing and sludge and deposit formation, while maintaining excellent shift quality throughout the duration of the field test.

Applications:

  • Heavy-duty automatic transmissions in trucks and buses in extended drain or severe service, such as in intracity transit buses, intercity tour coaches, school buses, emergency vehicles, recreational vehicles, refuse vehicles and commercial utility vehicles
Triton Heavy Duty ATF is OEM-approved for service fill in:
  • Allison automatic transmissions in off-highway applications where a C-4 fluid is specified (approval no. C4-32612008)
Triton Heavy Duty ATF is recommended for service fill in:
  • Allison automatic transmissions in on-highway applications where a TES-295 quality fluid is specified
  • Voith DIWA transmissions
  • ZF Ecomat transmissions
Features/Benefits:
  • Excellent friction durability for smooth shifting throughout the service interval
  • Outstanding oxidation resistance and thermal stability for long fluid life
  • Protects against sludge and varnish formation
  • Protects against wear
  • High shear stability
  • Protects against rust and corrosion
  • Outstanding low-temperature properties for easier shifting in cold weather
  • Good seal compatibility
  • Good foam resistance

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.846 g/cc0.846 g/cc
Density 0.844 g/cc0.0305 lb/in³
Brookfield Viscosity 7000 cP
@Temperature -40.0 °C
7000 cP
@Temperature -40.0 °F
Viscosity Measurement 193193Index
Kinematic Viscosity at 40°C (104°F) 34 cSt34 cSt
Kinematic Viscosity at 100°C (212°F) 7.4 cSt7.4 cSt
 
Thermal PropertiesMetricEnglishComments
Pour Point -55.0 °C-67.0 °F
Flash Point 230 °C446 °FCOC
 
Descriptive Properties
ColorRed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ChevronTexaco Havoline® MERCON®/DEXRON®-III Automatic Transmission Fluid
Phillips 66 Kendall® Classic ATF Transmission Fluid
Phillips 66 CVT Fluid Full-Synthetic Transmission Fluid
ELM® SoyFluid™ Hydraulic Universal Tractor Biodegradable Tractor Hydraulic-Transmission Fluid
ConocoPhillips Hydroclear® ATF Type F Automatic Transmission Fluid

WCON5442 / 198695

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.