MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Garlock GYLON® 3522 PTFE Diaphragm
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: GYLON PTFE diaphragm
  • Withstands aggressive chemicals and temperatures up to +500°F (+260°C).
  • Up to four times the flex life of conventional PTFE
  • Reduced void content - less permeation, increased life
  • Improved equipment efficiency
Media: Strong caustics, strong acids, hydrocarbons, chlorine and cryogenics.
Conforms to FDA regulations.

Information provided by Garlock Rubber Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 5000 psiASTM D1708
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
@Pressure 5.52 MPa
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Compressibility, %20-25ASTM F36
Creep Relaxation, %35ASTM F38

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dalau Dalcon 001 100% Virgin PTFE
Saint-Gobain Chemfab® 1580 PTFE Coated Fiberglass Conveyor Belting
Soarus SoarnoL® BG3522 Ethylene Vinyl Alcohol Copolymer
NeoGraf GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing
Beijing Evergrow Resources PTFE Sheet

PGARL817 / 157543

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.