MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dalau Dalcon 001 100% Virgin PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Applications & Industries:
General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.
Chemical: Dynamic & shaft seals; Pipes & tubing for carrying chemicals; and Seals & gaskets. Flat gaskets are used to seal flanges in pipelines.
Construction: Bridge bearings. Slide bearings.
Electrical: Communications, radio & television engineering, cable insulation; Electrical plant construction & electronics industry (connectors & terminals); General electrical equipment (P.T.F.E. excellent electrical insulating material); and Power plant installations (switchgear).
Engineering: Anti - friction bearing cages & bearing plates; Bearings and bushes; Diaphragm pumps. Film bearings. Multi - layer composite bearings. Fabric bearings; Laboratory equipment. Measuring & control technology; Pipe supports. Expansion bellows. Glandless valves & pumps, valve seats; Piston rings in hydraulic systems; and Piston rod packings used in compressor plunger pumps & valves.
Food: Dynamic & shaft seals (used in the food processing industry) and Linings & coatings (fertiliser plant & food industry line equipment).

CHEMICAL RESISTANCE: The strength of the carbon - fluorine bond and the shielding of the carbon chains by the fluorine atoms result in a chemical inertness which is virtually universal, except alkali metals, fluorine under certain conditions, and some fluorine compounds at elevated temperatures. Some Fluorinated Hydrocarbons (refrigerants) cause reversible swelling i.e. Tetrafluorodichloroethane Frigen 21, giving a 9.6% weight increase. For specific data on chemical resistance of this material we have a computer database with all the information covering over 90% of all known chemicals.

Information provided by Dalau

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.13 - 2.19 g/cc0.0770 - 0.0791 lb/in³BS2782:Pt6
Deformation 7.9 %7.9 %Permanent Deformation; ASTM D621
 10 %
@Time 3600 sec,
Pressure 5.00 MPa
10 %
@Time 1.00 hour,
Pressure 725 psi
150°C; ASTM D621
 11.8 %
@Time 3600 sec,
Pressure 14.2 MPa
11.8 %
@Time 1.00 hour,
Pressure 2060 psi
ASTM D621
 14.3 %
@Pressure 14.2 MPa,
Time 86400 sec
14.3 %
@Pressure 2060 psi,
Time 24.0 hour
ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 57 - 6457 - 64ASTM D2240
Tensile Strength 15.0 - 35.0 MPa2180 - 5080 psiMolding Direction; BS2782:Pt3
Elongation at Break 150 - 350 %150 - 350 %Molding Direction; BS2782:Pt3
Flexural Modulus 0.690 GPa100 ksiASTM D790
Compressive Modulus 0.600 - 0.700 GPa
@Strain 0.2 %
87.0 - 102 ksi
@Strain 0.2 %
ASTM D621
Coefficient of Friction, Dynamic 0.0600.060ASTM D1894
Coefficient of Friction, Static 0.0800.080ASTM D1894
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+18 ohm-cm1.00e+18 ohm-cmASTM D257
Surface Resistance 1.00e+17 ohm1.00e+17 ohmASTM D257
Dielectric Constant  2.1
@Frequency 60 Hz
2.1
@Frequency 60 Hz
ASTM D150
 2.1
@Frequency 1e+6 Hz
2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm610 kV/inOil(Molding); ASTM D149
 35.0 kV/mm889 kV/inOil (Extrusion); ASTM D149
 60.0 - 80.0 kV/mm1520 - 2030 kV/inAir (Tape); ASTM D149
Dissipation Factor  <= 0.00030
@Frequency 60 Hz
<= 0.00030
@Frequency 60 Hz
ASTM D150
 <= 0.00030
@Frequency 1e+6 Hz
<= 0.00030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 142 µm/m-°C
@Temperature 23.0 - 200 °C
78.9 µin/in-°F
@Temperature 73.4 - 392 °F
ASTM D696
CTE, linear, Transverse to Flow 153 µm/m-°C
@Temperature 23.0 - 200 °C
85.0 µin/in-°F
@Temperature 73.4 - 392 °F
ASTM D696
Thermal Conductivity 0.240 W/m-K1.67 BTU-in/hr-ft²-°FMolding Direction; ASTM C177
Melting Point 327 °C621 °FASTM D3417
Maximum Service Temperature, Air 260 °C500 °F
 300 °C572 °FShort Periods
Minimum Service Temperature, Air -200 °C-328 °F
Flash Point 530 °C986 °FASTM D1929
Oxygen Index >= 95 %>= 95 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Haze 80 - 85 %80 - 85 %ASTM D1003
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Isoflon Virgin PTFE Polytetrafluoroethylene
Polikim EFALON® T-100 Virgin PTFE
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
Syensqo (Solvay Specialty Polymers) Torlon® 4203 Polyamide-imide (PAI)

PDALAU001 / 132989

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.