MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dalau Dalcon 001 100% Virgin PTFE
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Applications & Industries:
General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.
Chemical: Dynamic & shaft seals; Pipes & tubing for carrying chemicals; and Seals & gaskets. Flat gaskets are used to seal flanges in pipelines.
Construction: Bridge bearings. Slide bearings.
Electrical: Communications, radio & television engineering, cable insulation; Electrical plant construction & electronics industry (connectors & terminals); General electrical equipment (P.T.F.E. excellent electrical insulating material); and Power plant installations (switchgear).
Engineering: Anti - friction bearing cages & bearing plates; Bearings and bushes; Diaphragm pumps. Film bearings. Multi - layer composite bearings. Fabric bearings; Laboratory equipment. Measuring & control technology; Pipe supports. Expansion bellows. Glandless valves & pumps, valve seats; Piston rings in hydraulic systems; and Piston rod packings used in compressor plunger pumps & valves.
Food: Dynamic & shaft seals (used in the food processing industry) and Linings & coatings (fertiliser plant & food industry line equipment).

CHEMICAL RESISTANCE: The strength of the carbon - fluorine bond and the shielding of the carbon chains by the fluorine atoms result in a chemical inertness which is virtually universal, except alkali metals, fluorine under certain conditions, and some fluorine compounds at elevated temperatures. Some Fluorinated Hydrocarbons (refrigerants) cause reversible swelling i.e. Tetrafluorodichloroethane Frigen 21, giving a 9.6% weight increase. For specific data on chemical resistance of this material we have a computer database with all the information covering over 90% of all known chemicals.

Information provided by Dalau

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.13 - 2.19 g/ccBS2782:Pt6
Deformation 7.9 %Permanent Deformation; ASTM D621
 10 %
@Time 3600 sec,
Pressure 5.00 MPa
150°C; ASTM D621
 11.8 %
@Time 3600 sec,
Pressure 14.2 MPa
ASTM D621
 14.3 %
@Pressure 14.2 MPa,
Time 86400 sec
ASTM D621
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 57 - 64ASTM D2240
Tensile Strength 15.0 - 35.0 MPaMolding Direction; BS2782:Pt3
Elongation at Break 150 - 350 %Molding Direction; BS2782:Pt3
Flexural Modulus 690 MPaASTM D790
Compressive Modulus 600 - 700 MPa
@Strain 0.2 %
ASTM D621
Coefficient of Friction, Dynamic 0.060ASTM D1894
Coefficient of Friction, Static 0.080ASTM D1894
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+18 ohm-cmASTM D257
Surface Resistance 1.00e+17 ohmASTM D257
Dielectric Constant 2.1
@Frequency 60 Hz
ASTM D150
 2.1
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mmOil(Molding); ASTM D149
 35.0 kV/mmOil (Extrusion); ASTM D149
 60.0 - 80.0 kV/mmAir (Tape); ASTM D149
Dissipation Factor <= 0.00030
@Frequency 60 Hz
ASTM D150
 <= 0.00030
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 142 µm/m-°C
@Temperature 23.0 - 200 °C
ASTM D696
CTE, linear, Transverse to Flow 153 µm/m-°C
@Temperature 23.0 - 200 °C
ASTM D696
Thermal Conductivity 0.240 W/m-KMolding Direction; ASTM C177
Melting Point 327 °CASTM D3417
Maximum Service Temperature, Air 260 °C
 300 °CShort Periods
Minimum Service Temperature, Air -200 °C
Flash Point 530 °CASTM D1929
Oxygen Index >= 95 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Haze 80 - 85 %ASTM D1003
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Isoflon Virgin PTFE Polytetrafluoroethylene
Polikim EFALON® T-100 Virgin PTFE
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber
DuPont Mobility and Materials Vespel® SP-1 ISO Polyimide
Syensqo (Solvay Specialty Polymers) Torlon® 4203 Polyamide-imide (PAI)

PDALAU001 / 132989

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.