MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Santoprene® 121-65W233 Thermoplastic Elastomer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner molding, end caps and special fixation applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable.

  • Designed for applications requiring excellent adhesion to vulcanized EPDM rubber.
  • Specially formulated to replace thermoset EPDM rubber in automotive glass run channel corner molding applications.
  • Designed for shorter processing time compared to thermoset EPDM rubber.
  • Used in sealing applications.

Information provided by Advanced Elastomer Systems

Key Words: EU 2003/11/EC; RoHS Compliant
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.920 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 65.12 in; ASTM D2240
 66Air at 212°F, 70 hr; ASTM D573
Tensile Strength at Break 727.5 psiAir at 212°F, 70 hr; ASTM D573
 750 psiAcross Flow; ASTM D412
Tensile Strength, Ultimate 290 psiAcross Flow; ASTM D412
Elongation at Break 536.9 %Air at 212°F, 70 hr; ASTM D573
 590 %Across Flow; ASTM D412
Compression Set 20 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 - 230 °C
 
Descriptive Properties
ColorBlack
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 121-70B230 Thermoplastic Elastomer
ExxonMobil Santoprene® 151-60 Thermoplastic Rubber
ExxonMobil Santoprene® 521-70 Thermoplastic Rubber
ExxonMobil Santoprene® 121-80B230 Thermoplastic Elastomer
ExxonMobil Santoprene® 201-73W228 Thermoplastic Rubber

PADVA062 / 22752

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.