System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
3M Scotch-Weld™ DP125 Gray Epoxy Adhesive
Categories:
Polymer
;
Adhesive
;
Thermoset
;
Epoxy
;
Epoxy Adhesive
Material Notes:
Scotch-Weld epoxy adhesive DP125 Gray is a filled, pigmented version of the Scotch-Weld epoxy adhesive DP125 Translucent and has similar performance and flexibility properties.
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Brookfield Viscosity
35000
-
75000
cP
Base, RVF #7 spindle, 20 rpm @ 27°C
45000
-
65000
cP
Accelerator, RVF #7 spindle, 20 rpm @ 27°C
Mechanical Properties
Original Value
Comments
Hardness, Shore D
70
ASTM D2240
Tensile Strength at Break
22.8
MPa
ASTM D882
Elongation at Break
125 %
ASTM D882
Shear Strength
60.0
psi
Overlap, Polypropylene
250
psi
Overlap, +3M Primer 3901
400
psi
Overlap, Glass, Borosilicate
520
psi
Overlap, ABS
550
psi
Overlap, Acrylic
750
psi
Overlap, PVC
880
psi
Overlap, Polycarbonate
900
psi
Overlap, Wood, Fir
1800
psi
Overlap, Fiberglass
1900
psi
Overlap, Cold Rolled Steel
2200
psi
Overlap, Sanded Aluminum
3400
psi
Overlap, Etched Aluminum
400
psi
@Temperature 82.0 °C
Overlap
450
psi
@Temperature 66.0 °C
Overlap
700
psi
@Temperature 49.0 °C
Overlap
3400
psi
@Temperature -55.0 °C
Overlap
4300
psi
@Temperature 21.0 °C
Overlap
Peel Strength
2.00
pli
180°
3.00
pli
180°
3.00
pli
180°
18.0
pli
180°
35.0
pli
180°
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+11
ohm-cm
ASTM D257
Dielectric Constant
6.3
@Frequency 1000 Hz
ASTM D150
Dielectric Strength
680
kV/in
@Thickness 0.762 mm
ASTM D149
Thermal Properties
Original Value
Comments
CTE, linear
98.0
µm/m-°C
@Temperature 5.00 - 20.0 °C
Below Tg
187
µm/m-°C
@Temperature 65.0 - 140 °C
Above Tg
Thermal Conductivity
0.151
W/m-K
@Thickness 6.35 mm,
Temperature 44.3 °C
Glass Transition Temp, Tg
12.0
°C
Onset
23.0
°C
Mid-Point
Processing Properties
Original Value
Comments
Cure Time
2.50
hour
Time to Handling Strength
7.00
hour
Full
Tack-Free Time
2.00
hour
Descriptive Properties
Appearance
Amber
Accelerator
Gray
Base
Gray
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive
3M Scotch-Weld™ DP620NS Structural Adhesive
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M 760 Hybrid Adhesive Sealant
PMM34622 / 169369
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.