MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Wacker Belsil® CM 3092 Cyclopentasiloxane -Dimethiconol Blend
Categories: Fluid; Polymer

Material Notes: BELSIL® CM 3092 is a blend of cyclopentasiloxane and a high-molecular dimethiconol. Due to its composition, it combines the properties of the low viscosity, volatile cyclopentasiloxane and the extremely high-viscosity dimethiconol. The excellent spreading of cyclopentasiloxane allows a good distribution of the high-viscosity conditioning agent dimethiconol.

Application: BELSIL® CM 3092 is used in hair-care and in skincare applications. Skin-care and skin-protection preparations containing BELSIL® CM 3092 impart a pleasant, supple feel to skin; it facilitates the distribution of the formulations and improves skin elasticity. At the same time, it forms a water-resistant but breathable protective barrier. This provides good substantivity and fixation of active ingredients. Use of BELSIL® CM 3092 in hair-care products yields sleek, shiny hair. Damaged hair regains a natural, healthy appearance. Wet and dry combability are improved, and further damage to the hair cuticles is prevented. It is also widely used in hair-tip fluids.

INCI name: Cyclopentasiloxane, Dimethiconol

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³
Viscosity 7500 cP7500 cPdynamic
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.3971.397
Transmission, Visible 90 %90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Active ingredients (%)15
Appearancecolorless, clear
Solubility4-Methylbenzylidene camphor1-10%
 Benzophenoe-3insoluble
 C12-15 alkyl benzoatesinsoluble
 C9-13 isoparaffin>10%
 Castor oilinsoluble
 Ethanolinsoluble
 Ethyl acetate>10%
 Ethylhexyl methoxycinnamate1-10%
 Ethylhexyl Salicylate>10%
 Glycerininsoluble
 Isopropanolinsoluble
 Isopropyl myristate>10%
 Lanolin oilinsoluble
 Mineral oil (high-viscosity)insoluble
 Mineral oil (low-viscosity)insoluble
 Octyl dodecanolinsoluble
 Oleyl alcoholinsoluble
 Oleyl oleateinsoluble
 Olive oilinsoluble
 Propylene glycolinsoluble
 Waterinsoluble
 Wheat germ oilinsoluble

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wacker Belsil® DM 6101 E Dimethiconol - Emulsion
Wacker Belsil® DM 3560 VP Dimethiconol - Emulsion
Wacker Belsil® DM 3112 VP Dimethiconol - Emulsion
Wacker Belsil® CM 740 Cyclopentasiloxane -Dimethiconol Blend
Wacker Powersoft® AE 66 Silicone Softener

PWACK9010 / 204539

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.