MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
JIS SKH10 Tungsten High Speed Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Used in high speed tool and cutting applications such as drills, milling processes, reamers, etc. Tungsten content promotes high temperature hardness and wear resistance. Quench via oil, air, or salt bath.

Key Words: JIS G4403(83) SKH10, SKH 10, SKH-10; Comparable to AISI T15, UNS T12015
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.19 g/cc(AISI T15)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell <= 285Bar Forging Annealed
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.90 µm/m-°C
@Temperature 20.0 - 200 °C
(AISI T15)
 11.0 µm/m-°C
@Temperature 20.0 - 425 °C
(AISI T15)
 11.5 µm/m-°C
@Temperature 20.0 - 540 °C
(AISI T15)
 
Processing PropertiesOriginal ValueComments
Processing Temperature 540 - 650 °CTempering (AISI T15)
 1205 - 1260 °CHardening (AISI T15)
Annealing Temperature 870 - 900 °C(AISI T15)
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 1.5 - 1.6 %
Chromium, Cr 3.8 - 4.5 %
Cobalt, Co 4.2 - 5.2 %
Copper, Cu <= 0.25 %
Iron, Fe 68.6 - 74.9 %As Balance
Manganese, Mn <= 0.40 %
Nickel, Ni <= 0.25 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 0.40 %
Sulfur, S <= 0.030 %
Tungsten, W 11.50 - 14 %
Vanadium, V 4.2 - 5.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Schmolz + Bickenbach Thermodur® 2343 EFS Extra Fine Structure (H-11)- Hot Work Die Steel
Carpenter Micro-Melt® T-15 Alloy (AISI T15)
Bohler-Uddeholm AISI D2 Cold Work Tool Steel
ATI Allegheny Ludlum AL 17-4 High Strength Stainless Steel, UNS S17400
AISI Type T15 Tungsten High Speed Tool Steel (UNS T12015)

MSTZJSKH10 / 231100

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.