MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Bohler-Uddeholm AISI D2 Cold Work Tool Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Tool Steel; Cold Work Steel

Material Notes: AISI D2 is a high-carbon, high-chromium tool steel alloyed with molybdenum and vanadium

AISI AD2 is characterized by:

  • High wear resistance
  • High compressive strength
  • Good through-hardening properties
  • High stability in hardening
  • Good resistance to tempering-back

Applications: AISI D2 is recommended for tools requiring very high wear resistance, combined with moderate toughness (shock-resistance). AISI D2 can be supplied in various finishes, including the hot-rolled, pre-machined and fine machined condition.

Key Words: AISI D2; W.-Nr. 1.2379
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.67 g/cc0.277 lb/in³hardened to 62 HRC
 7.61 g/cc
@Temperature 399 °C
0.275 lb/in³
@Temperature 750 °F
hardened to 62 HRC
 7.64 g/cc
@Temperature 199 °C
0.276 lb/in³
@Temperature 390 °F
hardened to 62 HRC
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 210210Soft annealed
Modulus of Elasticity 209.9 GPa30450 ksi(hardened to 62 HRC)
 180 GPa
@Temperature 399 °C
26100 ksi
@Temperature 750 °F
hardened to 62 HRC
 200 GPa
@Temperature 199 °C
29000 ksi
@Temperature 390 °F
hardened to 62 HRC
Compressive Yield Strength 1650 MPa239000 psi0.2%, hardened to 50 HRC
 1900 MPa276000 psi0.2%, hardened to 55 HRC
 2150 MPa312000 psi0.2%, hardened to 60 HRC
 2200 MPa319000 psi0.2%, hardened to 62 HRC
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.2 µm/m-°C
@Temperature 20.0 - 200 °C
6.20 µin/in-°F
@Temperature 68.0 - 392 °F
high temp. tempering, hardened to 62 HRC
 12.1 µm/m-°C
@Temperature 20.0 - 400 °C
6.70 µin/in-°F
@Temperature 68.0 - 752 °F
high temp. tempering, hardened to 62 HRC
 12.2 µm/m-°C
@Temperature 20.0 - 200 °C
6.80 µin/in-°F
@Temperature 68.0 - 392 °F
low temp. tempering, hardened to 62 HRC
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
0.110 BTU/lb-°F
@Temperature 68.0 °F
hardened to 62 HRC
Thermal Conductivity  20.0 W/m-K
@Temperature 20.0 °C
139 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
hardened to 62 HRC
 21.0 W/m-K
@Temperature 199 °C
146 BTU-in/hr-ft²-°F
@Temperature 390 °F
hardened to 62 HRC
 23.0 W/m-K
@Temperature 399 °C
160 BTU-in/hr-ft²-°F
@Temperature 750 °F
hardened to 62 HRC
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 1.55 %1.55 %
Chromium, Cr 11.8 %11.8 %
Iron, Fe 84.35 %84.35 %As Balance
Manganese, Mn 0.40 %0.40 %
Molybdenum, Mo 0.80 %0.80 %
Silicon, Si 0.30 %0.30 %
Vanadium, V 0.80 %0.80 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type D2 Tool Steel, air quenched at 1010°C, tempered at 200°C
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 450°C
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C
Crucible Steel AIRDI® 150 (AISI D2) Tool Steel
AISI Type A2 Tool Steel

NBUCOR21 / 15490

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.