Applications include high-speed screw machine products where superior machining characteristics of this steel can be fully utilized. |
UNS G12144, ASTM A29, ASTM A108, SAE J403, SAE J412, SAE J414, DIN 1,0718, UNI 9 SMnPb 23, JIS SUM 22 L, JIS SUM 24 L, SS14 1914 (Sweden) |