MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Covestro MAKROFOL® HF312 G-4 020021 Polycarbonate Films
Categories: Polymer; Film; Thermoplastic; Polycarbonate (PC)

Material Notes: Characterization: Makrofol HF 312 G-4 020021 is an extrusion film based on Makrolon® polycarbonate with a UV-curable hard coat on one side.

Properties / Applications: Makrofol HF 312 G-4 020021 is an extrusion film based on Makrolon® polycarbonate with a UV-curable hard coat on one side. The film can be printed on the uncoated side. The product can be shaped by thermoforming or high pressure forming (HPF). After forming, the hard coat must be cured by applying UV radiation to achieve scratch and chemical resistance. Makrofol HF 312 G-4 020021 is available in standard thickness of 0.0075" and 0.0105" (190 microns and 265 microns). Other thicknesses are available on request. The surface structure of Makrofol HF 312 G-4 020021 is one side gloss, one side fine matte. One side is protected with a PE-masking film. As with any product, use of Makrofol HF 312 G-4 020021 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccISO 1183, Method C
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 50.0 MPa>= 7250 psiISO 527-1,-3
Elongation at Break >= 100 %>= 100 %ISO 527-1,-3
Tensile Modulus 2.10 GPa305 ksiYoung's; ISO 527-1,-3
 
Optical PropertiesMetricEnglishComments
Gloss >= 80 %>= 80 %60; DIN EN ISO 2813

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro MAKROFOL® UV 244 6-2 040004 Polycarbonate Films
Covestro Makrofol® DE 7-2 Polycarbonate
Covestro Makrofol® BL 2-4 820816 Polycarbonate
Covestro Makrofol® DE 6-2 Polycarbonate
Covestro Makrofol® DE 1-4 000000 Polycarbonate

PCOVEST0805 / 202588

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.