Characterization: Makrofol HF 312 G-4 020021 is an extrusion film based on Makrolon® polycarbonate with a UV-curable hard coat on one side. Properties / Applications: Makrofol HF 312 G-4 020021 is an extrusion film based on Makrolon® polycarbonate with a UV-curable hard coat on one side. The film can be printed on the uncoated side. The product can be shaped by thermoforming or high pressure forming (HPF). After forming, the hard coat must be cured by applying UV radiation to achieve scratch and chemical resistance. Makrofol HF 312 G-4 020021 is available in standard thickness of 0.0075" and 0.0105" (190 microns and 265 microns). Other thicknesses are available on request. The surface structure of Makrofol HF 312 G-4 020021 is one side gloss, one side fine matte. One side is protected with a PE-masking film. As with any product, use of Makrofol HF 312 G-4 020021 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability. Information provided by Covestro |