MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Extrusion Coating  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Extrusion Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer designed for extrusion coating, laminating and seaming applications. It can be processed to 625°F and has excellent adhesive properties to substrates such as polypropylene, HDPE, PVdC, and paper.

Applications: Seaming; Heavy duty shipping sacks; Dunnage bags; Tarpaulins; Agricultural and construction films; Pond liners; Medical packages. Data for film properties below based on 1.25 mil film.

Key Words: EMA; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.928 g/ccExxon Method
Thickness 1.25 mil
Melt Flow 6.0 g/10 minExxon Method
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 290 %ASTM D882
Film Elongation at Break, TD 620 %ASTM D882
Secant Modulus, MD 0.120 GPaASTM D882
Secant Modulus, TD 0.140 GPaASTM D882
Coefficient of Friction 0.90ASTM D1894
Elmendorf Tear Strength MD 100 gASTM D1922
Elmendorf Tear Strength TD 70 gASTM D1922
Elmendorf Tear Strength, MD 80.0 g/milASTM D1922
Elmendorf Tear Strength, TD 56.0 g/milASTM D1922
Dart Drop 80.0 g/milF50; ASTM D1709
Dart Drop Test 100 gF50; ASTM D-1709
Film Tensile Strength at Break, MD 19.0 MPaASTM D882
Film Tensile Strength at Break, TD 19.0 MPaASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 102 °CExxon Method
 
Optical PropertiesOriginal ValueComments
Haze 11 %ASTM D1003
Gloss 44 %45°, ASTM D-2457

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Nucrel® 960 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin
Dow Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer

PEXCES / 37904

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.