MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow Nucrel® 699 Ethylene-Methacrylic Acid Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate

Material Notes: Nucrel® 599 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for exterior applications and painted or plated for special decorative effects.

Typical Applications:

  • Ink modification
  • Adhesive component
  • Special adhesive films

Features:

  • Higher deflection temperature
  • Good adhesion to metals and polar substrates

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM D792
Melt Index of Compound 95 g/10 min
@Load 2.16 kg,
Temperature 190 °C
95 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4646Initial (peak) hardness; ASTM D2240
Tensile Strength at Break 15.2 MPa2200 psiType IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638
Elongation at Break 560 %560 %Type IV specimen, compression molded, crosshead speed 2 in/min; ASTM D638
Flexural Modulus 0.0683 GPa9.91 ksiASTM D790
Izod Impact, Notched NBNBASTM D256
Tensile Impact Strength  288 kJ/m²
@Temperature -40.0 °C
137 ft-lb/in²
@Temperature -40.0 °F
ASTM D1822S
 491 kJ/m²
@Temperature 23.0 °C
234 ft-lb/in²
@Temperature 73.4 °F
ASTM D1822S
 
Thermal PropertiesMetricEnglishComments
Melting Point 80.0 - 94.0 °C176 - 201 °FASTM D3418(DSC)
Vicat Softening Point 65.0 °C149 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Zone 1 160 °C320 °F
Zone 2 182 °C360 °F
Zone 3 193 °C379 °F
Zone 4 204 °C399 °F
Zone 5 204 °C399 °F
Die Temperature 204 °C400 °F
Melt Temperature 149 - 232 °C300 - 450 °F
 
Descriptive Properties
Methacrylic Acid Content11 wt.%DuPont Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nucrel® 0411HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
DuPont Nucrel® 535 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 599 Ethylene-Methacrylic Acid Copolymer Resin
Dow Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin

PDUPM106 / 33773

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.