MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Nylon 6, Glass Bead Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Bead Filled

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.920 - 1.68 g/ccAverage value: 1.36 g/cc Grade Count:192
Filler Content 10.0 - 40.0 %Average value: 27.8 % Grade Count:9
Water Absorption 0.800 - 8.00 %Average value: 2.84 % Grade Count:39
Moisture Absorption at Equilibrium 0.250 - 3.00 %Average value: 1.92 % Grade Count:84
 2.00 - 2.10 %
@Temperature 70.0 - 70.0 °C
Average value: 2.08 % Grade Count:5
Water Absorption at Saturation 0.800 - 8.00 %Average value: 6.12 % Grade Count:43
Viscosity 2.90 - 3.20 cPAverage value: 2.99 cP Grade Count:9
Viscosity Test 145 - 150 cm³/gAverage value: 148 cm³/g Grade Count:4
Viscosity Number 140 cm³/gAverage value: 140 cm³/g Grade Count:3
Maximum Moisture Content 0.0200 - 0.150Average value: 0.141 Grade Count:15
 0.200 - 0.300
@Temperature 120 - 120 °C
Average value: 0.230 Grade Count:5
 0.200 - 0.300
@Time 299 - 299 sec
Average value: 0.230 Grade Count:5
Linear Mold Shrinkage 0.00100 - 0.0200 cm/cmAverage value: 0.00974 cm/cm Grade Count:140
 0.00500 - 0.00900 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00780 cm/cm Grade Count:10
Linear Mold Shrinkage, Transverse 0.00100 - 0.0197 cm/cmAverage value: 0.0105 cm/cm Grade Count:67
 0.00800 - 0.0100 cm/cm
@Temperature 80.0 - 80.0 °C
Average value: 0.00920 cm/cm Grade Count:10
Melt Flow 3.00 - 100 g/10 minAverage value: 35.5 g/10 min Grade Count:29
Ash 18.0 - 62.0 %
@Temperature 625 - 625 °C
Average value: 35.0 % Grade Count:4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 110 - 122Average value: 118 Grade Count:12
Hardness, Shore D 80.0 - 90.0Average value: 85.4 Grade Count:4
Ball Indentation Hardness 65.0 - 220 MPaAverage value: 139 MPa Grade Count:15
Tensile Strength, Ultimate 30.0 - 210 MPaAverage value: 73.3 MPa Grade Count:169
 20.0 - 45.0 MPa
@Temperature 60.0 - 150 °C
Average value: 31.3 MPa Grade Count:1
Tensile Strength, Yield 35.0 - 119 MPaAverage value: 75.2 MPa Grade Count:24
Elongation at Break 0.500 - 155 %Average value: 10.6 % Grade Count:176
 10.0 - 35.0 %
@Temperature 60.0 - 150 °C
Average value: 20.0 % Grade Count:1
Elongation at Yield 3.00 - 15.0 %Average value: 7.43 % Grade Count:14
 8.00 - 14.0 %
@Temperature 60.0 - 150 °C
Average value: 11.5 % Grade Count:1
Modulus of Elasticity 1.10 - 19.0 GPaAverage value: 4.29 GPa Grade Count:158
 0.580 - 2.00 GPa
@Temperature 60.0 - 150 °C
Average value: 1.10 GPa Grade Count:1
Flexural Yield Strength 10.3 - 340 MPaAverage value: 118 MPa Grade Count:114
Flexural Modulus 0.703 - 18.0 GPaAverage value: 4.16 GPa Grade Count:127
Flexural Strain at Break 2.50 - 7.50 %Average value: 4.80 % Grade Count:5
Izod Impact, Notched 0.160 - 1.28 J/cmAverage value: 0.497 J/cm Grade Count:27
Izod Impact, Unnotched 1.33 J/cm - NBAverage value: 5.18 J/cm Grade Count:19
Izod Impact, Notched (ISO) 2.50 - 20.0 kJ/m²Average value: 6.01 kJ/m² Grade Count:50
 2.00 - 42.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 9.36 kJ/m² Grade Count:14
Izod Impact, Unnotched (ISO) 20.0 kJ/m² - NBAverage value: 42.3 kJ/m² Grade Count:12
 20.0 - 75.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 41.1 kJ/m² Grade Count:7
Charpy Impact Unnotched 1.00 J/cm² - NBAverage value: 4.56 J/cm² Grade Count:139
 1.80 - 9.03 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 4.02 J/cm² Grade Count:59
Charpy Impact, Notched 0.200 - 3.36 J/cm²Average value: 0.681 J/cm² Grade Count:144
 0.100 - 1.50 J/cm²
@Temperature -40.0 - -20.0 °C
Average value: 0.427 J/cm² Grade Count:59
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+9 - 1.00e+17 ohm-cmAverage value: 4.17e+15 ohm-cm Grade Count:89
Surface Resistance 1.00e+10 - 1.00e+16 ohmAverage value: 3.59e+14 ohm Grade Count:71
Dielectric Constant 3.00 - 6.10Average value: 4.54 Grade Count:44
Dielectric Strength 7.87 - 80.0 kV/mmAverage value: 25.8 kV/mm Grade Count:58
Dissipation Factor 0.0150 - 0.210Average value: 0.0625 Grade Count:22
Dielectric Loss Index 0.0200 - 0.200Average value: 0.110 Grade Count:16
Comparative Tracking Index 250 - 600 VAverage value: 481 V Grade Count:54
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 - 90.0 µm/m-°CAverage value: 47.3 µm/m-°C Grade Count:30
CTE, linear, Transverse to Flow 60.0 - 90.0 µm/m-°CAverage value: 76.3 µm/m-°C Grade Count:8
Specific Heat Capacity 1.40 J/g-°CAverage value: 1.40 J/g-°C Grade Count:4
Thermal Conductivity 0.340 - 0.360 W/m-KAverage value: 0.344 W/m-K Grade Count:5
Melting Point 178 - 255 °CAverage value: 219 °C Grade Count:106
Maximum Service Temperature, Air 80.0 - 200 °CAverage value: 145 °C Grade Count:20
Deflection Temperature at 0.46 MPa (66 psi) 170 - 235 °CAverage value: 196 °C Grade Count:70
Deflection Temperature at 1.8 MPa (264 psi) 50.0 - 230 °CAverage value: 123 °C Grade Count:139
Deflection Temperature at 8.0 MPa 45.0 - 140 °CAverage value: 63.3 °C Grade Count:6
Vicat Softening Point 190 - 247 °CAverage value: 205 °C Grade Count:56
Minimum Service Temperature, Air -60.0 °CAverage value: -60.0 °C Grade Count:3
Flammability, UL94 HB - V-0Grade Count:101
Oxygen Index 22.0 - 31.0 %Average value: 24.6 % Grade Count:12
Glow Wire Test 650 - 960 °CAverage value: 704 °C Grade Count:22
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 271 °CAverage value: 225 °C Grade Count:13
Nozzle Temperature 210 - 293 °CAverage value: 256 °C Grade Count:6
Melt Temperature 220 - 302 °CAverage value: 265 °C Grade Count:137
Mold Temperature 40.0 - 120 °CAverage value: 79.4 °C Grade Count:134
Drying Temperature 60.0 - 100 °CAverage value: 81.2 °C Grade Count:108
Moisture Content 0.0300 - 0.200 %Average value: 0.142 % Grade Count:43
Dew Point -17.8 °CAverage value: -17.8 °C Grade Count:3
Injection Pressure 30.0 - 138 MPaAverage value: 89.0 MPa Grade Count:27

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 6, 30% Glass Fiber Filled
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
Overview of materials for Nylon 66, Unreinforced
Overview of materials for Nylon 6, Glass Filled, Impact Grade
Overview of materials for Nylon 6, MoS2 Filled

O2418 / 77978

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.