MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Crucible Steel 303 Plus Chromium-Nickel Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Crucible 303 Plus is a non-hardenable austenitic chromium-nickel steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 303 stainless is obtained by the use of modern manufacturing methods and stringent mill controls. This grade is non-magnetic in the annealed condition bt slightly magnetic when cold worked. Typical applications are screw machine products and all machined parts requiring good corrosion resistance or non-magnetic properties

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.92 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 170
Tensile Strength, Ultimate 90000 psi
Tensile Strength, Yield 35000 psi
@Strain 0.2 %
Elongation at Break 50 %in 2"
Reduction of Area 55 %
Tensile Modulus 28000 ksi
Izod Impact Unnotched 80.0 ft-lb
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000721 ohm-cm
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.60 µin/in-°F
@Temperature 0.000 - 100 °C
 9.90 µin/in-°F
@Temperature 0.000 - 316 °C
 10.4 µin/in-°F
@Temperature 0.000 - 649 °C
Specific Heat Capacity 0.120 BTU/lb-°F
@Temperature 0.000 - 100 °C
Thermal Conductivity 112.8 BTU-in/hr-ft²-°F
@Temperature 93.3 °C
 150 BTU-in/hr-ft²-°F
@Temperature 538 °C
Melting Point 2550 - 2590 °F
Solidus 2550 °F
Liquidus 2590 °F
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.15 %
Chromium, Cr 17 - 19 %
Iron, Fe >= 66.9 %As Remainder
Manganese, Mn <= 2.0 %
Molybdenum, Mo <= 0.60 %
Nickel, Ni 8.0 - 10 %
Phosphorus, P <= 0.20 %
Silicon, Si <= 1.0 %
Sulfur, S >= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 6061-T6; 6061-T651
Crucible Steel 303 SE Chromium-Nickel Steel
PSM Industries Pacific Sintered Metals FN-255-S Nickel Steel Powdered Metal (MPIF FN-0200-25)
Crucible Steel 304L Chromium-Nickel Steel
HP Alloys Nitronic® 60 Austenitic Stainless, Level 5 Cold Worked

NCRUC033 / 16026

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.