MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel 303 SE Chromium-Nickel Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T 300 Series Stainless Steel

Material Notes: Crucible 303 SE is a non-hardenable austenitic chromium-nickel steel to which selenium has been added to improve machinability and non-galling characteristics. This grade is non-magnetic in the annealed condition bt slightly magnetic when cold worked. Typical applications are screw machine products the will be subjected to cold forming.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 7.92 g/cc7.92 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 170170
Tensile Strength, Ultimate 621 MPa90000 psi
Tensile Strength, Yield 241 MPa
@Strain 0.2 %
35000 psi
@Strain 0.2 %
Elongation at Break 50 %50 %in 2"
Reduction of Area 55 %55 %
Tensile Modulus 193 GPa28000 ksi
Izod Impact Unnotched 108 J80.0 ft-lb
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000721 ohm-cm
@Temperature 23.0 °C
0.0000721 ohm-cm
@Temperature 73.4 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  17.3 µm/m-°C
@Temperature 0.000 - 100 °C
9.60 µin/in-°F
@Temperature 32.0 - 212 °F
 17.8 µm/m-°C
@Temperature 0.000 - 316 °C
9.90 µin/in-°F
@Temperature 32.0 - 600 °F
 18.7 µm/m-°C
@Temperature 0.000 - 649 °C
10.4 µin/in-°F
@Temperature 32.0 - 1200 °F
Specific Heat Capacity 0.502 J/g-°C
@Temperature 0.000 - 100 °C
0.120 BTU/lb-°F
@Temperature 32.0 - 212 °F
Thermal Conductivity  16.25 W/m-K
@Temperature 93.3 °C
112.8 BTU-in/hr-ft²-°F
@Temperature 200 °F
 21.6 W/m-K
@Temperature 538 °C
150 BTU-in/hr-ft²-°F
@Temperature 1000 °F
Melting Point 1400 - 1420 °C2550 - 2590 °F
Solidus 1400 °C2550 °F
Liquidus 1420 °C2590 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.12 %<= 0.12 %
Chromium, Cr 17 - 19 %17 - 19 %
Iron, Fe >= 66.76 %>= 66.76 %As Remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Molybdenum, Mo <= 0.60 %<= 0.60 %
Nickel, Ni 8.0 - 10 %8.0 - 10 %
Phosphorus, P 0.12 - 0.17 %0.12 - 0.17 %
Selenium, Se 0.15 - 0.35 %0.15 - 0.35 %
Silicon, Si <= 1.0 %<= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel 303 Plus Chromium-Nickel Steel
17-7 PH Stainless Steel, CH900, plate, sheet, and strip
AISI Type S21800 Stainless Steel
Crucible Steel 304L Chromium-Nickel Steel
PSM Industries Pacific Sintered Metals FN-255-S Nickel Steel Powdered Metal (MPIF FN-0200-25)

NCRUC034 / 16027

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.