MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Aluminum Alloys, General
Categories: Metal; Nonferrous Metal; Aluminum Alloy

Material Notes: These properties are typical of commercial aluminum alloys. Some properties, such as strength and hardness, vary too much for a reasonable generalization. See entries for individual alloys and heat treatments for more specific information. Aluminum 1199 is the highest purity (99.99% Al min.) in the database.

Aluminum is a silver-colored, low density (2.7 g/cc) metal that finds use in a huge variety of commercial applications. Unalloyed aluminum is ductile, exhibits moderate strength, and is very resistant to corrosion under most circumstances. Aluminum can be strengthened by the addition of appropriate alloying elements (Cu, Mg, Mn, Si, etc.) and subsequent heat/work treatments. Aluminum is commonly used in both wrought and cast forms.

The low density of aluminum results in its extensive use in the aerospace industry, and in other transportation fields. Its resistance to corrosion leads to its use in food and chemical handling (cookware, pressure vessels, etc.) and to architectural uses.

Key Words: Al Alloys
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.70 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 70.0 GPa
Poissons Ratio 0.33
Shear Modulus 26.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000500 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 390 J/g
CTE, linear 24.0 µm/m-°C
@Temperature 0.000 - 100 °C
 25.0 µm/m-°C
@Temperature 250 °C
Specific Heat Capacity 0.880 J/g-°C
Thermal Conductivity 190 W/m-K
Melting Point 620 - 650 °C
Solidus 620 °C
Liquidus 650 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 87 - 100 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Aluminum Alloy
Overview of materials for 6000 Series Aluminum Alloy
Aluminum, Al
Overview of materials for 2000 Series Aluminum Alloy
Overview of materials for 7000 Series Aluminum Alloy

MA0001 / 8714

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.