MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for 2000 Series Aluminum Alloy
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "2000 Series Aluminum Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.58 - 2.89 g/cc0.0932 - 0.104 lb/in³Average value: 2.79 g/cc Grade Count:190
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 45.0 - 15045.0 - 150Average value: 114 Grade Count:70
Hardness, Knoop 72.0 - 19172.0 - 191Average value: 147 Grade Count:55
Hardness, Rockwell A 36.9 - 53.636.9 - 53.6Average value: 46.5 Grade Count:52
Hardness, Rockwell B 49.0 - 88.049.0 - 88.0Average value: 73.7 Grade Count:55
Hardness, Vickers 81.0 - 21081.0 - 210Average value: 135 Grade Count:55
Tensile Strength, Ultimate 172 - 670 MPa25000 - 97200 psiAverage value: 405 MPa Grade Count:119
Tensile Strength, Yield 68.9 - 570 MPa10000 - 82700 psiAverage value: 309 MPa Grade Count:119
Elongation at Break 0.500 - 27.0 %0.500 - 27.0 %Average value: 8.85 % Grade Count:119
Creep Strength 315 - 470 MPa45700 - 68200 psiAverage value: 383 MPa Grade Count:3
Rupture Strength 420 - 485 MPa60900 - 70300 psiAverage value: 452 MPa Grade Count:3
Modulus of Elasticity 70.0 - 117 GPa10200 - 16900 ksiAverage value: 76.3 GPa Grade Count:119
Compressive Yield Strength 185 - 470 MPa26800 - 68200 psiAverage value: 397 MPa Grade Count:7
Compressive Modulus 73.8 - 78.0 GPa10700 - 11300 ksiAverage value: 75.2 GPa Grade Count:14
Notched Tensile Strength 379 - 414 MPa55000 - 60000 psiAverage value: 393 MPa Grade Count:5
Ultimate Bearing Strength 345 - 896 MPa50000 - 130000 psiAverage value: 786 MPa Grade Count:7
Bearing Yield Strength 131 - 696 MPa19000 - 101000 psiAverage value: 508 MPa Grade Count:7
Poissons Ratio 0.300 - 0.3400.300 - 0.340Average value: 0.327 Grade Count:84
Fatigue Strength 80.0 - 469 MPa11600 - 68000 psiAverage value: 164 MPa Grade Count:43
Fracture Toughness 19.0 - 49.0 MPa-m½17.3 - 44.6 ksi-in½Average value: 31.7 MPa-m½ Grade Count:12
Machinability 30.0 - 90.0 %30.0 - 90.0 %Average value: 67.9 % Grade Count:29
Shear Modulus 26.0 - 44.2 GPa3770 - 6410 ksiAverage value: 29.0 GPa Grade Count:83
Shear Strength 106 - 320 MPa15400 - 46400 psiAverage value: 248 MPa Grade Count:66
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000349 - 0.00000820 ohm-cm0.00000349 - 0.00000820 ohm-cmAverage value: 0.00000492 ohm-cm Grade Count:89
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.0 - 25.6 µm/m-°C8.89 - 14.2 µin/in-°FAverage value: 22.8 µm/m-°C Grade Count:112
Specific Heat Capacity 0.836 - 0.926 J/g-°C0.200 - 0.221 BTU/lb-°FAverage value: 0.869 J/g-°C Grade Count:78
Thermal Conductivity 84.0 - 200 W/m-K583 - 1390 BTU-in/hr-ft²-°FAverage value: 139 W/m-K Grade Count:105
Melting Point 502 - 670 °C935 - 1240 °FAverage value: 573 °C Grade Count:73
Solidus 502 - 560 °C935 - 1040 °FAverage value: 529 °C Grade Count:73
Liquidus 635 - 670 °C1180 - 1240 °FAverage value: 642 °C Grade Count:56
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 338 - 413 °C640 - 775 °FAverage value: 408 °C Grade Count:51
Solution Temperature 493 - 535 °C919 - 995 °FAverage value: 510 °C Grade Count:58
Aging Temperature 22.2 - 238 °C72.0 - 460 °FAverage value: 166 °C Grade Count:31
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 86.4 - 99.3 %86.4 - 99.3 %Average value: 93.5 % Grade Count:184
Beryllium, Be 0.000100 - 0.00500 %0.000100 - 0.00500 %Average value: 0.00122 % Grade Count:5
Bismuth, Bi 0.100 - 1.00 %0.100 - 1.00 %Average value: 0.362 % Grade Count:33
Chromium, Cr 0.0400 - 0.350 %0.0400 - 0.350 %Average value: 0.0973 % Grade Count:93
Copper, Cu 0.100 - 6.80 %0.100 - 6.80 %Average value: 3.96 % Grade Count:184
Iron, Fe 0.0500 - 1.50 %0.0500 - 1.50 %Average value: 0.454 % Grade Count:173
Lead, Pb 0.00300 - 2.00 %0.00300 - 2.00 %Average value: 0.516 % Grade Count:32
Lithium, Li 0.600 - 2.60 %0.600 - 2.60 %Average value: 1.57 % Grade Count:27
Magnesium, Mg 0.0200 - 2.20 %0.0200 - 2.20 %Average value: 0.760 % Grade Count:170
Manganese, Mn 0.0500 - 1.30 %0.0500 - 1.30 %Average value: 0.431 % Grade Count:164
Nickel, Ni 0.0500 - 2.30 %0.0500 - 2.30 %Average value: 0.664 % Grade Count:28
Oxygen, O 0.0500 - 0.600 %0.0500 - 0.600 %Average value: 0.519 % Grade Count:4
Si+Fe 0.400 - 0.700 %0.400 - 0.700 %Average value: 0.675 % Grade Count:12
Silicon, Si 0.0500 - 7.50 %0.0500 - 7.50 %Average value: 0.443 % Grade Count:173
Silver, Ag 0.0500 - 0.700 %0.0500 - 0.700 %Average value: 0.397 % Grade Count:18
Tin, Sn 0.0300 - 1.90 %0.0300 - 1.90 %Average value: 0.610 % Grade Count:16
Titanium, Ti 0.0100 - 0.300 %0.0100 - 0.300 %Average value: 0.127 % Grade Count:145
Vanadium, V 0.0500 - 0.150 %0.0500 - 0.150 %Average value: 0.0833 % Grade Count:24
Zinc, Zn 0.0500 - 1.30 %0.0500 - 1.30 %Average value: 0.298 % Grade Count:179
Zirconium, Zr 0.0400 - 0.500 %0.0400 - 0.500 %Average value: 0.141 % Grade Count:62
Zr+Ti 0.200 - 0.250 %0.200 - 0.250 %Average value: 0.237 % Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for 6000 Series Aluminum Alloy
Overview of materials for 5000 Series Aluminum Alloy
Overview of materials for 7000 Series Aluminum Alloy
Overview of materials for 3000 Series Aluminum Alloy
Overview of materials for 4000 Series Aluminum Alloy

M01041 / 81683

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.